High solids coatings for building panels

Inventors: John E. Hughes (Lincoln University, PA); Steven L Masia (Lancaster, PA)
Assignee: AWI Licensing LLC
C09D131/04C08K3/22C08K3/26C09D7/06C09D7/43C09D7/45C09D7/63E04C2/043C08K3/34C08K5/10C08K2003/2227C08K2003/2241C08K2003/265C08L2205/03E04C2002/005
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,898,049
App. No.
17/529,540
Filed
Nov 18, 2021
Granted
Feb 13, 2024
Kind
B2
Art Unit
1787
USPC
428/500
Abstract

Described herein is a coating composition suitable for application to a building panel. The coating composition comprises inorganic pigment, liquid carrier, and a humectant comprising a first ester-containing compound. The liquid carrier may be present in an amount ranging from about 10 wt. % to about 30 wt. % based on the total weight of the coating composition. Described herein are also building panels coated with the coating composition and methods of their production.

Claims (53)

1. A building system comprising:

a first building panel positioned adjacent to a second building panel, and a seam formed between the first and second building panels;

a seam-filling material applied to the seam;

a coating applied to the first and second building panels and the seam-filling material, the coating comprising:

a binder having a pH of at least about 7.0 and a Tg of at least 20° C.;

a pigment; and

a viscosity modifier;

wherein the pigment and the binder are present in a weight ratio of at least about 5:1;

wherein the viscosity modifier comprises a humectant and a dispersant; and

wherein the humectant and the dispersant are present in a weight ratio ranging from about 1:1 to about 4:1; and

wherein the pigment comprises titanium dioxide, calcium carbonate, alumina trihydrate, and diatomaceous earth.

2. The building system according to claim 1 , wherein the Tg of the binder is at least 30° C.

3. The building system according to claim 1 , wherein the binder is a styrene acrylic copolymer.

4. The building system according to claim 3 , wherein the styrene acrylic copolymer has a pH ranging from about 7.5 to about 9.

5. The building system according to claim 1 , wherein the binder is polyvinyl acetate.

6. The building system according to claim 5 , wherein the polyvinyl acetate has a pH of about 7.0.

7. The building system according to claim 1 , wherein the humectant is selected from the group consisting of ester-containing humectants including sugar-based esters and glycol-based esters.

8. The building system according to claim 1 , wherein the dispersant comprises an ionic dispersant.

9. The building system according to claim 1 , wherein the dispersant comprises a non-ionic dispersant.

10. The building system according to claim 1 , wherein the pigment and the binder are present in a weight ratio of at least 7:1.

11. The building system according to claim 1 , wherein the coating is applied in an amount ranging from about 10 g/ft 2 to about 70 g/ft 2 .

12. The building system according to claim 1 , wherein the seam-filling material comprises gypsum plaster.

13. The building system according to claim 1 ,

wherein each of the first and second building panels comprise a first major surface opposite a second major surface and a side surface extending between the first and second major surfaces, and the seam is located between adjacent side surfaces of the first and second building panel, and

wherein the seam-filling material is applied to a portion of the first major surface of the first building panel and a portion of the first major surface of the second building panel; and

wherein the coating is applied continuously across the first major surface of the first building panel, the seam-filling material, and the first major surface of the second building panel.

14. The building system according to claim 13 , wherein the first major surface of the first building panel has a first aesthetic appearance and the seam-filling material has a second aesthetic appearance, the first aesthetic appearance being different from the second aesthetic appearance, and wherein the coating substantially masks both the first and second aesthetic appearance.

15. The building system according to claim 14 , wherein the coating exhibits a maximum airflow resistance of about 1,000 MKS Rayls.

16. The building system according to claim 1 , wherein the humectant comprises at least one ester bond.

17. A building system comprising:

a first building panel and a second building panel, the first building panel positioned adjacent to the second building panel to form a seam between the first and second building panels;

a seam-filling material applied to the seam;

a coating applied to the first and second building panels and the seam-filling material, the coating comprising:

a binder;

a pigment blend comprising titanium dioxide, calcium carbonate, and diatomaceous earth; and

a viscosity modifier;

wherein the viscosity modifier comprises a humectant and a dispersant; and

wherein the humectant and the dispersant are present in a weight ratio ranging from about 1:1 to about 4:1; and

wherein the humectant comprises at least one ester bond.

18. The building system of claim 17 , wherein the coating is applied to a central region of each the first and second building panels, and wherein a surface of the central region of the first building panel is parallel with a surface of the central region of the second building panel.

19. The building system of claim 17 , wherein the binder has a pH of at least about 7.0 and a Tg of at least 20° C.

20. A building system comprising:

a plurality of building panels having at least a first building panel and a second building panel;

a coating over the first building panel and the second building panel; and

a seam-filling material between the first building panel and the second building panel;

the coating comprising:

a binder;

a pigment blend comprising titanium dioxide, calcium carbonate, and diatomaceous earth; and

a viscosity modifier;

wherein the viscosity modifier comprises a humectant and a dispersant;

wherein the humectant and the dispersant are present in a weight ratio ranging from about 1:1 to about 4:1;

wherein the pigment and the binder are present in a weight ratio of at least about 7:1; and

wherein the binder comprises styrene acrylic copolymer or polyvinyl acetate.