Optical film, display device using the same, composition for forming colored layer used for producing optical film
Provided are an optical film that can reduce reflectance, increase luminance, reduce thickness, and improve color reproducibility a display device, and a display device using the same. An optical film characterized by comprising a transparent substrate, a colored layer laminated on one surface side of the transparent substrate and containing a dye, and a functional layer laminated on the other surface side of the transparent substrate, wherein the dye contains a first coloring material having a maximum absorption wavelength of 470 to 530 nm and a half width of the absorption spectrum of 15 to 45 nm, and a second coloring material having a maximum absorption wavelength of 560 to 620 nm and a half width of the absorption spectrum of 15 to 55 nm, and the transparent substrate has an ultraviolet shielding rate of 85% or more according to JIS L 1925.
1 . An optical film comprising
a transparent substrate,
a colored layer laminated on one surface side of the transparent substrate and including a dye, and
a functional layer laminated on the other surface side of the transparent substrate, wherein
the dye includes
a first coloring material having a maximum absorption wavelength in the range of 470 to 530 nm and a half width of the absorption spectrum of 15 to 45 nm, and
a second coloring material having a maximum absorption wavelength in the range of 560 to 620 nm and a half width of the absorption spectrum of 15 to 55 nm,
and, wherein
the transparent substrate has an ultraviolet shielding rate of 85% or more according to JIS L 1925,
the first coloring material is a pyrromethene cobalt complex, and
the colored layer includes a hindered amine light stabilizer having a molecular weight of 2000 or more.
2 . The optical film according to claim 1 , wherein the surface has a pencil hardness of H or higher under a load of 500 g.
3 . The optical film according to claim 1 , wherein the colored layer includes at least one of a peroxide decomposer or a singlet oxygen quencher.
4 . The optical film according to claim 3 , wherein the singlet oxygen quencher included in the colored layer is a transition metal complex of dialkyl phosphate, dialkyldithiocarbamate or benzenedithiol or similar dithiol.
5 . The optical film according to claim 1 , wherein the colored layer further includes, as the dye, a third coloring material having a maximum absorption wavelength within the range of 650 to 800 nm.
6 . The optical film according to claim 1 , wherein the dye included in the colored layer includes one or more compounds selected from the group consisting of compounds having any one of a porphyrin structure, a merocyanine structure, a phthalocyanine structure, an azo structure, a cyanine structure, a squarylium structure, a coumarin structure, a polyene structure, a quinone structure, a tetraazaporphyrin structure, a pyrromethene structure and an indigo structure and metal complexes thereof.
7 . The optical film according to claim 1 , further comprising an oxygen barrier layer having an oxygen permeability of 10 cc/(m 2 *day*atm) or less between the transparent substrate and the colored layer or on the other side of the transparent substrate.
8 . The optical film according to claim 1 , wherein the functional layer comprises an antireflection layer including a high refractive index layer and a low refractive index layer, or an antiglare layer.
9 . The optical film according to claim 1 , further comprising an antistatic layer or an antifouling layer.
10 . A display device comprising the optical film according to claim 1 .
11 . A composition for forming colored layer comprising an active energy ray-curable resin, a photopolymerization initiator, a dye, an additive, and a solvent,
wherein
the dye includes
a first coloring material having a maximum absorption wavelength in the range of 470 to 530 nm and a half width of the absorption spectrum of 15 to 45 nm, and
a second coloring material having a maximum absorption wavelength in the range of 560 to 620 nm and a half width of the absorption spectrum of 15 to 55 nm, wherein
the first coloring material is a pyrromethene cobalt complex, and
the additive contains a hindered amine light stabilizer having a molecular weight of 2000 or more.