Wound core
This wound core is a wound core including a wound core main body obtained by stacking a plurality of polygonal annular grain-oriented electrical steel sheets in a side view, and the grain-oriented electrical steel sheet has planar portions and bent portions that are alternately continuous in a longitudinal direction, and in at least one bent portion, the crystal grain size Dpx (mm) of the grain-oriented electrical steel sheet is FL/4 or more. Here, FL the an average length (mm) of the planar portions.
1 . A wound core including a wound core main body obtained by stacking a plurality of polygonal annular grain-oriented electrical steel sheets in a sheet thickness direction in a side view,
wherein the grain-oriented electrical steel sheet has planar portions and bent portions that are alternately continuous in a longitudinal direction,
wherein the bent portion in a side view has an inner radius of curvature r of 1 mm or more and 5 mm or less,
wherein the grain-oriented electrical steel sheets have a chemical composition containing,
in mass %,
Si: 2.0 to 7.0%, with the remainder comprising Fe and impurities, and
have a texture oriented in the Goss orientation, and
in at least one of the bent portions, the crystal grain size Dpx (mm) of the stacked grain-oriented electrical steel sheet is FL/4 or more,
where Dpx (mm) is an average value of Dp obtained by the following Formula (1),
Dc (mm) is an average crystal grain size in a direction in which a boundary line extends at respective boundaries between the bent portion and two planar portions arranged with the bent portion therebetween,
Dl (mm) is an average crystal grain size in a direction perpendicular to a direction in which the boundary line extends at the boundary,
FL (mm) is an average length of a shorter planar portion between two adjacent planar portions with the bent portion therebetween, and
the average value of Dp is an average value of Dp on the inner side and Dp on the outer side of one planar portion between two planar portions and Dp on the inner side and Dp on the outer side of the other planar portion:
Dp
=
√
(
Dc
×
Dl
/
π
)
.
(
1
)
2 . A wound core including a wound core main body obtained by stacking a plurality of polygonal annular grain-oriented electrical steel sheets in a sheet thickness direction in a side view,
wherein the grain-oriented electrical steel sheet has planar portions and bent portions that are alternately continuous in a longitudinal direction,
wherein the bent portion in a side view has an inner radius of curvature r of 1 mm or more and 5 mm or less,
wherein the grain-oriented electrical steel sheets have a chemical composition containing,
in mass %,
Si: 2.0 to 7.0%, with the remainder comprising Fe and impurities, and
have a texture oriented in the Goss orientation, and
in at least one of the bent portions, the crystal grain size Dpy (mm) of the stacked grain-oriented electrical steel sheet is FL/4 or more,
where Dpy (mm) is an average value of Dl (mm),
Dl (mm) is an average crystal grain size in a direction perpendicular to a direction in which a boundary line extends at respective boundaries between the bent portion and two planar portions arranged with the bent portion therebetween,
FL (mm) is an average length of a shorter planar portion between two adjacent planar portions with the bent portion therebetween, and
the average value of Dl is an average value of Dl on the inner side and Dl on the outer side of one planar portion between two planar portions and Dl on the inner side and Dl on the outer side of the other planar portion.
3 . A wound core including a wound core main body obtained by stacking a plurality of polygonal annular grain-oriented electrical steel sheets in a sheet thickness direction in a side view,
wherein the grain-oriented electrical steel sheet has planar portions and bent portions that are alternately continuous in a longitudinal direction,
wherein the bent portion in a side view has an inner radius of curvature r of 1 mm or more and 5 mm or less,
wherein the grain-oriented electrical steel sheets have a chemical composition containing,
in mass %,
Si: 2.0 to 7.0%, with the remainder comprising Fe and impurities, and
have a texture oriented in the Goss orientation, and
in at least one of the bent portions, the crystal grain size Dpz (mm) of the stacked grain-oriented electrical steel sheet is FL/4 or more,
where Dpz (mm) is an average value of Dc (mm),
Dc (mm) is an average crystal grain size in a direction in which a boundary line extends at respective boundaries between the bent portion and two planar portions arranged with the bent portion therebetween,
FL (mm) is an average length of a shorter planar portion between two adjacent planar portions with the bent portion therebetween, and
the average value of Dc is an average value of Dc on the inner side and Dc on the outer side of one planar portion between two planar portions and Dc on the inner side and Dp on the outer side of the other planar portion.