IP Library Granted Patent US 12683209
Granted Patent B2
US 12683209 · App. 18/436,405 · Granted Jul 14, 2026

Battery treatment method

Inventors: Takayuki Sakata (Wako, JP); Yushi Fujinaga (Wako, JP); Mitsumasa Sorazawa (Wako, JP); Hideki Matsuda (Wako, JP); Satoru Takahashi (Wako, JP); Ryo Shimizu (Wako, JP)
Assignee: HONDA MOTOR CO., LTD.
H01M10/54C22B1/005
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12683209
App. No.
18/436,405
Granted
Jul 14, 2026
Kind
B2
Abstract

A method of treating a battery having a laminated electrode that includes a positive electrode plate and a negative electrode plate with a separator interposed between the positive electrode plate and the negative electrode plate, the battery being either a lithium ion battery or a solid-state battery, includes: an immersion step of immersing the laminated electrode in water after lithium is deactivated; and a separation step of separating the laminated electrode by applying an electrical pulse to the laminated electrode.

Claims (12)

1 . A method of treating a battery having a laminated electrode that includes a positive electrode plate and a negative electrode plate with a separator interposed between the positive electrode plate and the negative electrode plate, the battery being either a lithium ion battery or a solid-state battery, the method comprising:

an immersion step of immersing the laminated electrode in water after lithium is deactivated; and

a separation step of separating the laminated electrode by applying an electrical pulse to the laminated electrode, wherein

the electrical pulse is applied to the laminated electrode after the electrode plates of the laminated electrode are brought into an electrically connected state in the separation step,

the electrode plates of the laminated electrode are brought into the electrically connected state by penetration of a predetermined electrical connection member into the laminated electrode in the separation step,

the battery includes a positive electrode side current collector tab connected with the positive electrode plate and a negative electrode side current collector tab connected with the negative electrode plate, the negative electrode side current collector tab being disposed on an opposite side of the laminated electrode from the positive electrode side current collector tab, and

the electrical pulse is applied to the laminated electrode via the positive electrode side current collector tab and the negative electrode side current collector tab with the laminated electrode penetrated by the electrical connection member in a region near the negative electrode side current collector tab.

2 . A method of treating a battery having a laminated electrode that includes a positive electrode plate and a negative electrode plate with a separator interposed between the positive electrode plate and the negative electrode plate, the battery being either a lithium ion battery or a solid-state battery, the method comprising:

an immersion step of immersing the laminated electrode in water after lithium is deactivated; and

a separation step of separating the laminated electrode by applying an electrical pulse to the laminated electrode, wherein

the battery is a laminated battery having the laminated electrode covered with a laminate material with a pair of current collector tabs being exposed outside of the laminate material, and

the electrical pulse is applied to the laminated electrode via the pair of current collector tabs.