IP Library Granted Patent US 12692169
Granted Patent B2
US 12692169 · App. 18/010,994 · Granted Jul 28, 2026

Hollow inorganic particle and method for producing said hollow inorganic particle

Inventors: Hidenori Miyoshi (Tokyo, JP); Tatsuya Nakano (Tokyo, JP)
Assignee: UBE EXSYMO CO., LTD.
C01B33/18C01P2004/34C01P2004/61C01P2004/62
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12692169
App. No.
18/010,994
Granted
Jul 28, 2026
Kind
B2
Abstract

Provided is a hollow inorganic particle having excellent strength despite having high porosity. Provided is a hollow inorganic particle including an outer shell, the thinnest part of the outer shell/the thickest part of the outer shell being 0.80 or more. The hollow inorganic particle according to the present technology can be produced by a production method including: a coating step of coating core particles made of an organic polymer with a silicone-based compound; and a core particle removal step of removing the core particles. The coating step includes: a dispersant addition step of adding a dispersant to a core particle dispersion; and, after the dispersant addition step, a surfactant addition step of adding a cationic surfactant.

Claims (9)

1 . A method for producing hollow inorganic particles, comprising:

a coating step of coating core particles made of an organic polymer with a silicon-based compound; and

a core particle removal step of removing the core particles,

the coating step including:

a dispersant addition step of adding a nonionic surfactant as dispersant to a core particle dispersion; and,

after the dispersant addition step, a surfactant addition step of adding a cationic polymeric surfactant,

whereby the hollow inorganic particles thus produced have an average particle inner diameter/particle outer diameter of 0.55 to 0.93.

2 . The method for producing hollow inorganic particle according to claim 1 , wherein in the coating step, the core particle dispersion after the surfactant addition step has a cationic polymeric surfactant concentration of 0.05 to 5 g/L.

3 . The method for producing hollow inorganic particle according to claim 1 , wherein the dispersant is a hydrophilic polymer.