Packaged negative electrode material, method for transporting negative electrode material, container for storing negative electrode material, method for storing negative electrode material, and method for manufacturing negative electrode
A packaged negative electrode material, comprising a container and a negative electrode material contained in the container, the container having a water vapor transmission rate of 150 g/(m 2 ·d)(40° C./90% RH) or less, and the negative electrode material having a micropore volume of 0.40×10 −3 m 3 /kg or less.
1 . A packaged negative electrode material, comprising a container and a negative electrode material contained in the container,
the container having a water vapor transmission rate of 150 g/(m 2 ·d)(40 C°/90% RH) or less, and
the negative electrode material having a micropore volume of 0.40×10 −3 m 3 /kg or less.
2 . The packaged negative electrode material according to claim 1 , wherein the container has a volume of from 6000 cm 3 to 40000 cm 3 .
3 . The packaged negative electrode material according to claim 1 , wherein a filling ratio of the negative electrode material in the container is from 20% to 90%.
4 . The packaged negative electrode material according to claim 1 , wherein the negative electrode material is a negative electrode material for a lithium ion secondary battery.
5 . The packaged negative electrode material according to claim 1 , wherein the container comprises polyethylene.
6 . The packaged negative electrode material according to claim 1 , wherein the container is deformable.
7 . A method for transporting a negative electrode material, the method comprising transporting the packaged negative electrode material according to claim 1 .
8 . The method for transporting a negative electrode material according to claim 7 , wherein a manner of transportation is marine transport.
9 . A method for manufacturing a negative electrode, the method comprising:
extracting the negative electrode material from the container of the packaged negative electrode material according to claim 1 ; and
manufacturing a negative electrode using the negative electrode material extracted from the container.
10 . The method for manufacturing a negative electrode according to claim 9 , wherein the extracting the negative electrode material from the container and the manufacturing a negative electrode using the negative electrode material extracted from the container are conducted consecutively.
11 . A method for storing a negative electrode material, the method comprising storing a negative electrode material in a container,
the container having a water vapor transmission rate of 150 g/(m 2 ·d)(40 C°/90% RH) or less, and
the negative electrode material having a micropore volume of 0.40×10 −3 m 3 /kg or less.