Electron transport layer composition for inkjet printing and method for preparing same
An electron transport layer composition for inkjet printing is described. The composition includes metal oxide nanoparticles and at least three solvents being different in terms of at least one of viscosity, polarity, or vapor pressure. A method for preparing the composition and a light-emitting device having an electron transport layer formed from the composition are also described.
1 . An electron transport layer composition for inkjet printing, comprising:
metal oxide nanoparticles; and
at least three solvents that differ in terms of at least one of viscosity, polarity, or vapor pressure,
wherein the composition is capable of being ejected by ink-jetting; and
wherein the composition has a viscosity of 1.0 to 3.0 cps at 20° C. a vapor pressure of 0.6 to 45 mmHg at 20° C., a contact angle of 25 to 80°, and a solid content of 5 to 30 wt %.
2 . The composition of claim 1 , wherein the at least three solvents include dimethyl sulfoxide (DMSO), ethanol, 2-methoxy ethanol, and butanol.
3 . The composition of claim 2 , wherein a mixing ratio of the dimethyl sulfoxide (DMSO), ethanol, 2-methoxy ethanol, and butanol is a volume ratio of 3-8:1-3:1-2:0-1.
4 . The composition of claim 1 , wherein the metal oxide nanoparticles are Zn-containing metal oxide nanoparticles.
5 . The composition of claim 4 , wherein in the Zn-containing metal oxide nanoparticles, a metal capable of increasing a ZnO band gap is alloyed.
6 . The composition of claim 4 , wherein the Zn-containing metal oxide nanoparticles are ZnMgO.
7 . The composition of claim 1 , wherein the metal oxide nanoparticles have an organic ligand having hydrophilic moieties attached to a portion of or an entire surface thereof.
8 . The composition of claim 7 , wherein the organic ligand includes at least two hydrophilic moieties selected from a carboxyl group and a hydroxyl group.
9 . The composition of claim 7 , wherein the organic ligand is contained in a range of 0.0001 to 10 mol relative to 1 mol of a metal included in the metal oxide nanoparticles.
10 . The composition of claim 1 , wherein the metal oxide nanoparticles include a polymer coating layer formed on a portion of or an entire surface thereof.
11 . A light-emitting device, comprising:
a first electrode;
a second electrode disposed to face the first electrode;
an emission layer disposed between the first electrode and the second electrode;
a hole transport layer disposed between the first electrode and the emission layer; and
an electron transport layer disposed between the emission layer and the second electrode, the electron transport layer comprising:
metal oxide nanoparticles; and
at least three solvents that differ in terms of at least one of viscosity, polarity, or vapor pressure;
wherein the electron transport layer has a viscosity of 1.0 to 3.0 cps at 20° C. a vapor pressure of 0.6 to 45 mmHg at 20° C., a contact angle of 25 to 80°, and a solid content of 5 to 30 wt %.
12 . The light-emitting device of claim 11 , wherein the electron transport layer is formed by inkjet printing.
13 . The light-emitting device of claim 11 , wherein the light-emitting device further comprises at least one of a hole injection layer or an electron injection layer.
14 . The light-emitting device of claim 11 , wherein the at least three solvents include dimethyl sulfoxide (DMSO), ethanol, 2-methoxy ethanol, and butanol.
15 . The light-emitting device of claim 14 , wherein a mixing ratio of the dimethyl sulfoxide (DMSO), ethanol, 2-methoxy ethanol, and butanol is a volume ratio of 3-8:1-3:1-2:0-1.
16 . A method for preparing an electron transport layer composition for inkjet printing, the method comprising:
a first step of adding a basic substance to a reaction solution, in which a zinc-containing compound and a compound containing a metal capable of increasing a ZnO band gap are dissolved, followed by precipitation, thereby preparing a metal oxide nanoparticle dispersion; and
a second step of adding, to the prepared metal oxide nanoparticle dispersion, the at least three solvents that differ in terms of at least one of viscosity, polarity, or vapor pressure, followed by mixing, thereby preparing the electron transport layer composition;
wherein the electron transport layer composition has a viscosity of 1.0 to 3.0 cps at 20° C. a vapor pressure of 0.6 to 45 mmHg at 20° C. a contact angle of 25 to 80°, and a solid content of 5 to 30 wt %.
17 . The method of claim 16 , wherein the metal oxide nanoparticle dispersion in the first step further contains an organic ligand, the organic ligand being contained in a content of 10 wt % or less relative to 100 wt % of the metal oxide nanoparticle dispersion.
18 . The method of claim 16 , wherein the electron transport layer composition prepared in the second step further contains a monomer, the monomer being contained in a content of 10 vol % or less relative to 100 vol % of the electron transport layer composition.