IP Library Granted Patent US 12703168
Granted Patent B2
US 12703168 · App. 18/364,224 · Granted Aug 11, 2026

Reflective glass displays and associated methods for manufacturing reflective glass displays

Inventor: Kyle Fragassi (Pittsburgh, PA)
Assignee: Pittsburgh Glass Works, LLC
B32B3/04B32B7/12B32B17/10036B32B17/1077B32B17/10871B32B37/003B32B37/06B32B37/10G02F1/16757G02F1/1677B32B2305/34B32B2315/08B32B2375/00G02F2001/1678
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12703168
App. No.
18/364,224
Granted
Aug 11, 2026
Kind
B2
Abstract

A glass article includes a first glass substrate having a No. 1 surface and a No. 2 surface opposite the No. 1 surface, a second glass substrate opposed from the first glass substrate, the second glass substrate having a No. 3 surface that faces towards the No. 2 surface and a No. 4 surface opposite the No. 3 surface, and a display positioned between the first glass substrate and the second glass substrate.

Claims (13)

1 . A method for manufacturing a laminated glass article comprising a first glass substrate, a second glass substrate opposed from the first glass substrate, a first interlayer positioned between the first glass substrate and the second glass substrate, and a second interlayer positioned between the second glass substrate and the first interlayer, the method comprising:

positioning a middle interlayer between the first interlayer and the second interlayer to yield a stacked article;

removing air from the stacked article for a predetermined period of time;

heating the stacked article to a temperature between approximately 200° F. and approximately 300° F. for a second predetermined period of time;

heating the stacked article to a second temperature between approximately 200° F. and approximately 300° F. for a third predetermined period of time; and

subjecting the stacked article to a pressure between approximately 150PSI and approximately 200PSI for a fourth predetermined period of time.

2 . The method of claim 1 , wherein the one or more of the first interlayer, the second interlayer, and the middle interlayer comprises polyurethane.

3 . The method of claim 1 , wherein the predetermined period of time is about 10 minutes to about 30 minutes.

4 . The method of claim 1 , wherein the second predetermined period of time is about 15 minutes to about 45 minutes.

5 . The method of claim 1 , wherein the third predetermined period of time is about 20 minutes to about 40 minutes.

6 . The method of claim 1 , wherein the fourth predetermined period of time is approximately the same as the third predetermined period of time.

7 . The method of claim 1 , wherein the temperature is between approximately 220° F. and approximately 260° F.

8 . The method of claim 1 , wherein the second temperature is between approximately 220° F. and approximately 250° F.