Hydrophobic and oleophobic coating, preparation method therefor, and product
Disclosed are a hydrophobic and oleophobic coating, a preparation method therefor and a product, wherein the hydrophobic and oleophobic coating is formed by the deposition of a perfluoropolyether or perfluoropolyether derivative on the surface of a substrate by means of PECVD, such that the hydrophobic and oleophobic properties of the surface of the substrate are improved by the perfluoropolyether or perfluoropolyether derivative coating. Further disclosed are a hydrophobic and oleophobic coating, a preparation method therefor and a product, wherein the hydrophobic and oleophobic coating comprises: at least a two-layer structure, one of the layers being formed by the plasma chemical vapor deposition of one or more perfluoropolyethers or perfluoropolyether derivatives as raw materials, and the other layer being formed by the plasma chemical vapor deposition of a silane- or siloxane-containing raw material, thereby improving the hydrophobic and oleophobic properties of the surface of a substrate.
1 . A hydrophobic and oleophobic coating, formed by plasma enhanced chemical vapor deposition (PECVD) on a surface of a substrate with a perfluoropolyether derivative or a mixture of perfluoropolyether and a perfluoropolyether derivative as a raw material, wherein the perfluoropolyether derivative is a perfluoropolyether having at least one hydroxyl group or a perfluoropolyether having at least one carboxyl or ester group.
2 . The hydrophobic and oleophobic coating according to claim 1 , wherein the perfluoropolyether includes structural formulas of K-type, Y-type, Z-type, or D-type structures.
3 . The hydrophobic and oleophobic coating according to claim 1 , wherein the perfluoropolyether has a formula X 1 —O(CFXO) n (CFXCFXO) m (CF 2 CF 2 CF 2 O) p (CF 2 CF 2 CF 2 CF 2 O) q —X 2 (I), wherein —X 1 , X 2 are independently selected from structural formulas —(CF 2 ) Z CF 3 and CF(CF 3 )COF, wherein z is an integer from 0 to 3; X is the same or different at each occurrence, and is independently For CF 3 , n is an integer from 0 to 200; m is an integer from 0 to 200; p, q are integers from 0 to 100; p+q+m+n>0, and a number average molecular weight of (I) is between 200 and 10,000.
4 . The hydrophobic and oleophobic coating according to claim 1 , wherein the perfluoropolyether derivative is a perfluoropolyether hydroxyl derivative (PFPE-OH) having at least one hydroxyl group, the derivative PFPE-OH conforms to a formula T 1 -O—Rf-T 2 , wherein Rf is a fluoropolyoxyalkylene chain, T 1 and T 2 are the same as or different from each other and are independently selected from formulas —CF 2 CH 2 O(CH 2 CH 2 O) s ′H and —CF 2 CF 2 CH 2 O(CH 2 CH 2 O) s ″H, and wherein s′ and s″ are integers from 0 to 5.
5 . The hydrophobic and oleophobic coating according to claim 4 , wherein the fluoropolyoxyalkylene chain Rf of the derivative PFPE-OH is a chain comprising repeating units R o selected from: (i) —CFXO—, wherein X is F or CF 3 , (ii) —CFXCFXO—, wherein X is the same or different F or CF 3 at each occurrence, provided that at least one X is —F, (iii) —CF 2 CF 2 CF 2 O—, (iv) —CF 2 CF 2 CF 2 CF 2 O—, and (v) —(CF 2 ) j —CFZ—O—, wherein j is an integer from 0 to 3 and Z is a group having a general formula —ORf′T 3 , wherein Rf′ is a fluoropolyoxyalkylene chain comprising from 0 to 10 numbers of repeating units, and T 3 is a C 1 -C 3 perfluoroalkyl group.
6 . The hydrophobic and oleophobic coating according to claim 5 , wherein the repeating unit in Rf′ is selected from a group consisting of: —CFXO—, —CF 2 CFXO—, —CF 2 CF 2 CF 2 O—, and —CF 2 CF 2 CF 2 CF 2 O—, wherein each X is independently F or CF 3 .
7 . The hydrophobic and oleophobic coating according to claim 1 , wherein a temperature range of the vapor deposition is 30-60° C.
8 . A preparation method for a hydrophobic and oleophobic coating, comprising: with a perfluoropolyether derivative or a mixture of a perfluoropolyether and a perfluoropolyether derivative as a raw material, forming the hydrophobic and oleophobic coating on a surface of a substrate by plasma enhanced chemical vapor deposition (PECVD), wherein the perfluoropolyether derivative is a perfluoropolyether having at least one hydroxyl group or a perfluoropolyether having at least one carboxyl or ester group.
9 . The preparation method for the hydrophobic and oleophobic coating according to claim 8 , wherein a preparation process of the hydrophobic and oleophobic coating is: (1) placing the substrate in a reaction chamber of a plasma chamber, and vacuumizing the reaction chamber to reach a vacuum degree of 10-200 mtorr; (2) introducing a plasma source gas, turning on a pretreatment plasma discharge to pretreat the substrate, (3) vaporizing the raw material, introducing the raw material into the reaction chamber, turning on a deposition plasma discharge to perform the chemical vapor deposition; (4) turning off the deposition plasma discharge, introducing compressed air or inert gas to restore normal pressure, opening the chamber, and taking out the substrate.
10 . The preparation method for the hydrophobic and oleophobic coating according to claim 9 , wherein the raw material and the plasma source gas is introduced at the same time, or the substrate is first subjected to 1-1800s pretreatment after the plasma source gas is introduced before feeding the raw material.
11 . The preparation method for the hydrophobic and oleophobic coating according to claim 9 , wherein the pretreatment plasma discharge and the deposition plasma discharge are both performed by a pulse bias power supply in a constant power mode.
12 . A hydrophobic and oleophobic coating, comprising: at least two layers, wherein one layer is formed by plasma enhanced chemical vapor deposition with a perfluoropolyether derivative or a mixture of a perfluoropolyether and a perfluoropolyether derivative raw material, and another layer is formed by plasma enhanced chemical vapor deposition with a silane- or siloxane-containing raw material, wherein the perfluoropolyether derivative is a perfluoropolyether having at least one hydroxyl group or a perfluoropolyether having at least one carboxyl or ester group.
13 . The hydrophobic and oleophobic coating according to claim 12 , wherein a layer adjacent to a substrate surface is formed by plasma enhanced chemical vapor deposition with the silane- or siloxane-containing raw material.
14 . The hydrophobic and oleophobic coating according to claim 12 , wherein an outer layer is formed by plasma enhanced chemical vapor deposition of the perfluoropolyether derivative or the mixture of the perfluoropolyether and the perfluoropolyether derivative raw material.
15 . The hydrophobic and oleophobic coating according to claim 12 , wherein the silane- or siloxane-containing raw material is one or more selected from a group consisting of: vinyltrichlorosilane, 3-(methacryloyloxy) propyltrimethoxysilane, γ-aminopropyl triethoxysilane, γ-(2,3-glycidoxy) propyltrimethoxysilane, 3-aminopropyltrimethoxysilane, N-β-(aminoethyl)-γ-aminopropyl trimethoxysilane, N-β-(aminoethyl)-γ-aminopropylmethyldimethoxysilane, vinyltriethoxysilane, vinyltris(β-methoxyethoxy) silane, tetramethoxysilane, tetraethoxysilane, tetrapropoxysilane, allyltrimethoxysilane, hexamethyldisiloxane, tetramethyldisiloxane, hexaethyldisiloxane, 1,1,3,3-tetramethyldisiloxane, hexamethylcyclohexasiloxane, dodecamethylcyclohexasiloxane, octamethylcyclotetrasiloxane, decamethylcyclopentasiloxane, hexamethylcyclotrisiloxane, and hexadecylcyclooctasiloxane.
16 . The hydrophobic and oleophobic coating according to claim 12 , wherein the perfluoropolyether derivative has a formula HO—CH 2 CF 2 O(CF 2 O) m (CF 2 CF 2 O) n CF 2 CH 2 —OH, wherein m and n are integers.
17 . The hydrophobic and oleophobic coating according to claim 12 , wherein the perfluoropolyether derivative has a formula HO—(CH 2 CH 2 O) k CH 2 CF 2 O(CF 2 O) m (CF 2 CF 2 O) n CF 2 CH 2 (OCH 2 CH 2 ) k —OH, wherein m and n are integers and k=1 or 2.
18 . The hydrophobic and oleophobic coating according to claim 12 , wherein the perfluoropolyether has a formula CF 3 O(CF 2 —CF(CF 3 )O) n (CF 2 O) m CF 3 , wherein n/m=20, and has a number average molecular weight of 450.
19 . The hydrophobic and oleophobic coating according to claim 12 , wherein the perfluoropolyether has a formula CF 3 O(C 3 F 6 O) n (CF 2 O) m CF 3 , wherein/m=20.
20 . The hydrophobic and oleophobic coating according claim 12 , wherein the hydrophobic and oleophobic coating is suitable for deposition on a surface of a fabric material selected from a group consisting of: nylon, polyester fiber, acrylic fiber, and cotton.
21 . The hydrophobic and oleophobic coating according claim 12 , wherein the hydrophobic and oleophobic coating is suitable for deposition on a surface of a fabric containing 70% or more nylon material or a clothing fabric containing 60% or more cotton material.
22 . The hydrophobic and oleophobic coating according claim 12 , wherein the at least two layers are formed by successive multiple times of depositions during preparation.