IP Library Granted Patent US 8,034,153
Granted Patent B2
US 8,034,153 · App. 11/614,293 · Granted Oct 11, 2011

Wear resistant low friction coating composition, coated components, and method for coating thereof

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,034,153
App. No.
11/614,293
Filed
Dec 21, 2006
Granted
Oct 11, 2011
Kind
B2
Art Unit
1731
USPC
106/36
Abstract

A composition for coating sliding or rolling or fretting or impacting members is formed by preparing a composite powder of TiB2 and BN, with a TiB 2 to BN ratio ranging from 1:7 to 20:1, and a metallic matrix selected from the group consisting of nickel, chromium, iron, cobalt, aluminum, tungsten, carbon and alloys thereof.

Claims (26)

1. A coating composition for use on a contact surface, comprising 5 to 60 wt % total of composite powder having an average primary particle size ranging from 1 to 1000 μm, the balance comprising (i) a matrix-forming metal, metal alloy or high-temperature polymer, and (ii) a binder chosen from an acrylate resin, a methacrylate resin, a thermally cured phosphate binder, a thermally cured potassium silicate binder, or mixtures of two or more thereof; wherein the composite powder comprises TiB 2 and BN in a ratio of BN to TiB 2 of 1:7 to 20:1.

2. The coating composition of claim 1 , wherein the composite powder has a BET surface area of 0.1 to 20.0 m 2 /g.

3. The coating composition of claim 2 , wherein the composite powder has a BET surface area of 0.3 to 7.0 m 2 /g.

4. The coating composition of claim 1 , wherein the matrix-forming metal alloy is an alloy selected from the group consisting of W, Co, Cr, Fe, Ni, Mo, Al, Si, Cu, Y, Ag, P, Zr, Hf, B, Ta, V, Nb, and alloys thereof.

5. The coating composition of claim 1 , wherein the matrix-forming metal is selected from the group consisting of Ni, Co, Fe and alloys thereof.

6. The coating composition of claim 1 , wherein the matrix-forming high-temperature polymer is selected from the group consisting of polyimides, polyamide imides, polyester imides, aromatic plastics, and mixtures thereof.

7. The coating composition of claim 1 , wherein the matrix-forming metal alloy further comprises a high-temperature polymer selected from the group consisting of polyimides, polyamide imides, polyester imides, aromatic plastics, and mixtures thereof, in an amount of 1 to about 30 wt % of the composition.

8. The coating composition of claim 1 , wherein the composite powder comprises TiB 2 and BN in a ratio of BN to TiB 2 of 1:6 to 9:1.

9. The coating composition of claim 8 , wherein the composite powder comprises TiB 2 and BN in a ratio of BN to TiB 2 of 1:5 to 8:1.

10. The coating composition of claim 1 , wherein the composite powder has an average primary particle size ranging from 10 to 800 μm.

11. The coating composition of claim 10 , wherein the composite powder has an average primary particle size ranging from 20 to 500 μm.

12. The coating composition of claim 1 , wherein the composite powder has an average primary particle size ranging from 3 to 10 μm.

13. The coating composition of claim 1 , wherein the composite powder has a mechanical strength of >50 MPa.

14. The coating composition of claim 1 , wherein the composite powder is generated from one of scrapped metallization boats, scrapped side dams, and mixtures thereof.

15. The coating composition of claim 1 , wherein the composite powder is from scrapped materials containing:

10-60 wt. % BN;

1 to 60 wt. % of TiB 2 ;

0 to 60 wt. % of at least one of a nitride of the elements Al, Si, Fe, Co, Ni and mixtures thereof; and

30-70 wt. % of at least a material selected from the group of borides of Ti, Zr, Al, Cr and mixtures thereof, carbides of Si, Ti, and Cr and mixtures thereof.

16. The coating composition of claim 1 , wherein the composite powder is from scrapped materials containing:

TiB 2 , and BN, at least one of aluminum nitride or silicon nitride;

at least a metal selected from W, Fe, Co, Nb, Mo, Hf, V and Ta; and

at least an oxide selected from the group of CaO, MgO, Al 2 O 3 , TiO 2 , Y 2 O 3 , YAG (Al 5 Y 3 O 12 ), YAP(AlYO 3 ), and YAM(Al 2 Y 4 O 7 ), compounds and mixtures thereof.

17. The coating composition of claim 1 , wherein the composite powder further comprises at least one of nickel, chromium, iron, cobalt, aluminum and alloys thereof.

18. A coating composition for use on a contact surface, the composition comprising:

a compound powder mixture comprising a metallic matrix selected from the group consisting of nickel, chromium, iron, cobalt, aluminum, tungsten and alloys thereof, a binder chosen from an acrylate resin, a methacrylate resin, a thermally cured phosphate binder, a thermally cured potassium silicate binder, or mixtures of two or more thereof, and a composite powder of TiB 2 and BN; wherein the metallic component is present from 40 to 95 wt. % of the final coating composition and the TiB 2 to BN ratio in the composite powder of TiB 2 and BN is in the range of 1:7 to 20:1.