IP Library Granted Patent US 9,168,714
Granted Patent B2
US 9,168,714 · App. 13/538,085 · Granted Oct 27, 2015

Methods for making paperboard blanks and paperboard products therefrom

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,168,714
App. No.
13/538,085
Filed
Jun 29, 2012
Granted
Oct 27, 2015
Kind
B2
Art Unit
3728
USPC
220/62.22
Abstract

Methods for making paperboard blanks and paperboard products therefrom are provided. In one aspect, a method for making a paperboard blank can include burning a paperboard substrate to form at least one aperture therethrough. The method can also include securing a film onto a first side of the paperboard substrate to produce a paperboard blank.

Claims (44)

1. A paperboard product, comprising:

a sidewall formed from a paperboard blank; and

a bottom panel secured to the sidewall, wherein the sidewall comprises:

an inner surface comprising a film; and

an outer surface comprising a paperboard substrate, wherein the paperboard substrate has at least one aperture formed therethrough, and wherein the at least one aperture is formed by burning a portion of the paperboard substrate.

2. The paperboard product of claim 1 , wherein the paperboard substrate is burned with a laser beam.

3. The paperboard product of claim 1 , wherein the film is a shrinkable film.

4. The paperboard product of claim 3 , wherein the shrinkable film comprises a biaxially oriented heat shrinkable polymeric material.

5. The paperboard product of claim 1 , wherein the sidewall further comprises a brim formed by curling a first edge of the sidewall.

6. The paperboard product of claim 1 , wherein the film is secured to the paperboard substrate with an adhesive.

7. The paperboard product of claim 1 , wherein the paperboard substrate comprises at least a first outer layer, a second outer layer, and an intermediate layer, wherein the first and second outer layers comprise polyethylene, and wherein the intermediate layer comprises a paperboard.

8. The paperboard product of claim 7 , wherein the film is secured to the paperboard substrate by heat sealing the film to the paperboard substrate.

9. The paperboard product of claim 1 , wherein the at least one aperture has a cross-sectional area of about 0.005 mm 2 to about 1 mm 2 .

10. A method for making a paperboard product, comprising:

burning a paperboard substrate to form at least one aperture therethrough;

securing a film onto the paperboard substrate to produce a paperboard blank;

forming the paperboard blank to overlap two opposing edges of the paperboard blank to form a sidewall, wherein the sidewall comprises:

an inner surface comprising the film,

an outer surface comprising the paperboard substrate, and

a first edge adapted to be curled to form a brim curl, and

securing a bottom panel to the sidewall at or adjacent a second edge of the sidewall; and

curling the first edge of the sidewall to form the brim curl.

11. The method of claim 10 , wherein the paperboard substrate is burned with a laser beam.

12. The method of claim 10 , wherein the film is a shrinkable film.

13. The method of claim 10 , wherein the film is secured to the paperboard substrate with an adhesive.

14. The method of claim 10 , wherein burning the paperboard substrate completely removes a portion of the substrate to form the at least one aperture.

15. The method of claim 10 , wherein the at least one aperture has a cross-sectional area of about 0.005 mm 2 to about 1 mm 2 .

16. The method of claim 10 , wherein the film is a shrinkable film, and wherein the sidewall and the bottom panel define a product volume adapted to contain a liquid, the method further comprising selecting a shrinkable film in which an area of the shrinkable film decreases in an amount of about 10% to about 40% when a liquid at a temperature of up to about 100° C. is introduced into the product volume.

17. The method of claim 10 , wherein the film is a shrinkable film, and wherein the sidewall and the bottom panel define a product volume adapted to contain a liquid, the method further comprising selecting a shrinkable film that will shrink when a liquid at a temperature of about 70° C. to about 100° C. is introduced into the product volume, and wherein the outer surface of the sidewall remains at a temperature of about 44° C. or less after the liquid is introduced to the product volume.

18. The method of claim 10 , wherein the film is a shrinkable film, the method further comprising selecting a shrinkable film that shrinks when contacted with a fluid at a temperature of about 70° C. to about 100° C. to provide a paperboard container having a shrunk film and a gap located between at least a portion of the shrunk film and the paperboard substrate.

19. A paperboard product, comprising:

a sidewall formed from a paperboard blank; and

a bottom panel secured to the sidewall,

wherein the sidewall comprises:

an inner surface comprising a shrinkable film; and

an outer surface comprising at least a first outer layer, a second outer layer, and an intermediate layer, wherein the first and second outer layers comprise polyethylene, and the intermediate layer comprises a paperboard,

wherein the sidewall has at least one aperture formed therethrough, and the at least one aperture is formed by burning a portion of the sidewall, and wherein the shrinkable film shrinks at a temperature of at least 70° C. to provide a gap between at least a portion of the shrunk film and the outer surface.

20. The paperboard product of claim 19 , wherein the sidewall is burned with a laser beam to form the at least one aperture.

21. The paperboard product of claim 19 , wherein the shrinkable film comprises a biaxially oriented heat shrinkable polymeric material.

22. The paperboard product of claim 19 , wherein the sidewall further comprises a brim formed by curling a first edge of the sidewall.

23. The paperboard product of claim 19 , wherein the film is secured to the outer surface of the sidewall with an adhesive.

24. The paperboard product of claim 19 , wherein the film is secured to the outer surface of the sidewall by heat sealing the film to the outer surface.

25. The paperboard product of claim 19 , wherein the at least one aperture has a cross-sectional area of about 0.005 mm 2 to about 1 mm 2 .

26. The paperboard product of claim 19 , wherein the at least one aperture is located near a top of the sidewall.