IP Library Granted Patent US 6,949,488
Granted Patent B2
US 6,949,488 · App. 10/251,928 · Granted Sep 27, 2005

Fischer-Tropsch catalyst regeneration

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,949,488
App. No.
10/251,928
Granted
Sep 27, 2005
Kind
B2
Abstract

Methods and apparatus for providing the heat required to maintain the desired temperature for catalyst regeneration. The catalyst is heated by contacting a reactant gas mixture with the catalyst in order to initiate an exothermic reaction and, once the desired temperature is achieved, exposing the catalyst to a regenerating gas. The temperature may also be maintained by heating the reactant gas mixture prior to contacting the catalyst and/or adding a liquid, which may be heated, to the catalyst. For heating a Fischer-Tropsch catalyst for regeneration, the reactant gas preferably contains less than 12 mole percent carbon monoxide and more preferably contains between 1 and 4 mole percent carbon monoxide.

Claims (26)

1. A method of heating a catalyst for regeneration comprising;

contacting a reactant gas mixture with the catalyst to initiate an exothermic reaction so as to heat the catalyst, wherein the reactant gas comprises carbon monoxide and hydrogen and contains less than 12 mole percent of carbon monoxide; and

exposing the catalyst to a regenerating gas while the catalyst is heated by the exothermic reaction.

2. The method of claim 1 further comprising heating the reactant gas mixture prior to contacting the catalyst.

3. The method of claim 1 further comprising adding a liquid to the catalyst.

4. The method of claim 3 , wherein at least a portion of the added liquid is a liquid hydrocarbon stream having a boiling point at operating pressure such that the 5% point of the true boiling point (TBP) curve of the added liquid is higher than the temperature at which the catalyst is exposed to the regenerating gas.

5. The method of claim 3 further comprising heating the liquid before adding to the catalyst.

6. The method of claim 1 wherein the regenerating gas comprises a portion of the reactant gas.

7. A method of heating a Fischer-Tropsch catalyst for regeneration comprising;

contacting a reactant gas containing carbon monoxide and hydrogen with the catalyst to initiate a Fischer-Tropsch reaction and heat the catalyst, wherein the reactant gas contains less than 12 mole percent carbon monoxide; and

exposing the catalyst to a regenerating gas while the catalyst is heated by the Fischer-Tropsch reaction.

8. The method of claim 7 further comprising heating the reactant gas prior to contacting the catalyst.

9. The method of claim 7 further comprising adding liquid hydrocarbons to the catalyst.

10. The method of claim 9 further comprising heating the liquid hydrocarbons before adding to the catalyst.

11. The method of claim 9 , wherein at least a portion of the added liquid hydrocarbons have a boiling point at operating pressure such that the 5% point of the true boiling point (TBP) curve of the added liquid is higher than the temperature at which the catalyst is exposed to the regenerating gas.

12. The method of claim 7 wherein the reactant gas contains hydrogen.

13. The method of claim 7 wherein the reactant gas contains between 1 and 4 mole percent carbon monoxide.

14. The method of claim 7 wherein the catalyst is suspended in a slurry.

15. The method of claim 14 further comprising:

moving the slurry from a reactor vessel to a regenerating vessel;

regenerating the catalyst; and

moving the catalyst to the reactor vessel from the regenerating vessel.

16. The method of claim 15 wherein the slurry from the reactor vessel is at a temperature between 400° F. and 500° F.

17. The method of claim 15 wherein regenerating the catalyst takes place in the regenerating vessel at a temperature between 550° F. and 600° F.

18. The method of claim 7 wherein the catalyst is regenerated within a reactor vessel.

19. The method of claim 18 wherein the catalyst is regenerated within said reactor vessel by cycling between reaction mode and a regeneration mode.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 15, 2012
From: CONOCOPHILLIPS COMPANY
To: PHILLIPS 66 COMPANY
Reel/Frame 028213/0824 →
MERGER Recorded Feb 25, 2005
From: CONOCO INC.
To: CONOCOPHILLIPS COMPANY
Reel/Frame 015795/0508 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 9, 2002
From: BELT, BARBARA A.; LANDIS, STEPHEN R.; MOHEDAS, SERGIO R.; RAJE, AJOY P.
To: CONOCO INC.
Reel/Frame 013556/0468 →