IP Library Granted Patent US 6,869,505
Granted Patent B2
US 6,869,505 · App. 10/257,885 · Granted Mar 22, 2005

Method for calendering a board web

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,869,505
App. No.
10/257,885
Granted
Mar 22, 2005
Kind
B2
Abstract

A long nip (N) shoe calender formed of a shoe roll ( 10 ) and a thermo roll ( 20 ) is used in calendering, with a nip dwell time which is over 10 ms, advantageously over 20 ms. The nip pressure is below 3 MPa, advantageously below 1 MPa, and a surface temperature of the thermo roll ( 20 ) is over 200° C., advantageously over 250° C. The board web (W) surface to be pressed against the thermo roll ( 20 ) is moisturized before the nip.

Claims (7)

1. A method for calendaring an uncoated board web for manufacture of board grades White Lined Chipboard (WLC) and Folding Box Board (FBB) in a long nip shoe calendar, the method comprising the steps of:

passing the web at a first speed through a long nip shoe calender having a long nip formed between a shoe roll and a thermo roll, the long nip having a length such that the dwell time of the web within the nip is greater than 10 ms, and applying a nip pressure below 3 MPa, and wherein a surface temperature of the thermo roll is greater than 200° C., and wherein a calender belt having a hardness of below 100 ShA is used on the shoe roll; and

moisturizing the board web surface to be pressed against the thermo roll before the nip by spraying atomized water onto said board web surface in an amount of 1-20 g/m 2 such that the time of action of the water before the nip is about 0.1-2 s.

2. The method of claim 1 wherein the nip dwell time is greater than 20 ms.

3. The method of claim 1 wherein the nip pressure is below 1 MPa.

4. The method of claim 1 wherein the surface temperature of the thermo roll is greater than 250° C.

5. The method of claim 1 wherein the hardness of the calender belt is below 80 ShA.

Assignments (2)
CHANGE OF NAME Recorded Mar 27, 2014
From: METSO PAPER, INC.
To: VALMET TECHNOLOGIES, INC.
Reel/Frame 032551/0426 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 24, 2003
From: LARES, MATTI; TANI, MIKKO
To: METSO PAPER, INC.
Reel/Frame 014069/0324 →