Apparatus, mask, and method for printing alignment layer
View Patent ↗An apparatus for printing an alignment layer of a liquid crystal display device includes a dispenser dropping an alignment material, an anilox roll receiving the dropped alignment material, a doctor roll evenly spreading the dropped alignment material coated onto the anilox roll, and a printing roll receiving the alignment material from the anilox roll, and transferring the alignment material onto a substrate, wherein the printing roll has a plurality of masks each having a numerical aperture of about 5% to 25%.
1. A method for printing an alignment layer of a liquid crystal display device, comprising:
preparing an alignment material;
dropping the alignment material onto a doctor roll and an anilox roll by a dispenser;
printing the alignment material onto a substrate by using a printing roll having at least one mask with a numerical aperture of about 5% to about 25%; and
curing the alignment material printed on the substrate.
2. The method according to claim 1 , further comprising a step of forming an even thickness of the alignment material on the anilox roll by rotating the doctor roll and the anilox roll.
3. The method according to claim 1 , wherein curing the alignment material includes curing the alignment material at a first temperature range for a first time period, and curing the alignment material at a second temperature range for a second time period.
4. The method according to claim 3 , wherein the first temperature range is lower than the second temperature range.
5. The method according to claim 4 , wherein the second time period is longer than the first time period.
6. The method according to claim 1 , wherein curing the alignment material includes curing the alignment material at a temperature range of about 60° C. to about 80° C. for a first time period, and curing the alignment material at a temperature range of about 80° C. to about 250° C. for a second time period.
7. The method according to claim 6 , wherein the second time period is longer than the first time period.
8. The method according to claim 1 , wherein the at least one mask includes a plurality of masks each with a numerical aperture of about 5% to about 25%.
9. A mask for printing an alignment layer of a liquid crystal display device comprising a plurality of protrusions, wherein a numerical aperture of the mask is about 5% to about 25%.
10. The mask according to claim 9 , wherein a height of the protrusions is about 0.75 mm from a lower surface of the mask.
11. The mask according to claim 10 , wherein a total thickness of the mask is about 2.09 mm.
12. The mask according to claim 9 , wherein the mask is one of a printing rubber plate and a APR rubber plate.