Nitrile rubber mixtures with a low tendency towards mold contamination
View Patent ↗The present invention relates to a process for reducing mold contamination in an injection molding process by using a mixture of nitrile rubbers, in the range of from 0.1-0.5 wt. % of fatty acids and optionally further additives.
1. Process for reducing mold contamination in the injection molding process of a nitrile rubber, comprising the step of injecting a mixture comprising one or more nitrile rubbers and in the range of from 0.1-0.5 wt. % of a fatty acid(s) and optionally further additives and/or fillers into a mold.
2. Process according to claim 1 , wherein the nitrile rubber(s) is/are chosen from the group consisting of NBR, partly hydrogenated NBR, completely hydrogenated NBR and mixtures of two or more of the group members.
3. Process according claim 1 , wherein the fatty acid is a straight-chain fatty acid.
4. Process according to claim 1 , wherein the fatty acid is a fatty acid having 16 or 18 carbon atoms or a mixture of these.
5. Process according claim 1 , wherein the mixture further comprises a sillcatic filler, carbon black, zinc oxide, magnesium oxide or a mixture of two or more of these components.
6. Process according to claim 1 , wherein the mixture comprises vulcanization retardants and/or vulcanization accelerators.
7. Process for preparing a shaped article comprising the step of reducing mold contamination in the injection molding process of a nitrile rubber, by employing a mixture comprising or more nitrile rubbers and in the range of from 0.1-0.5 wt. % of a fatty acid(s) and optionally further additives and/or fillers.