IP Library Granted Patent US 7,045,028
Granted Patent B2
US 7,045,028 · App. 10/360,360 · Granted May 16, 2006

Composite and absorbent article comprising ultrasonics-friendly adhesive, and method of making same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,045,028
App. No.
10/360,360
Granted
May 16, 2006
Kind
B2
Abstract

The present invention is directed to reducing the build up or accretion of adhesive, alone or in combination with other materials, on the surfaces of equipment used to ultrasonically treat a workpiece (e.g., ultrasonically bonding various components or pieces to one another.) Thus the invention encompasses composites, absorbent products, and methods of making said composites and products where an adhesive composition having certain identified properties is used to reduce the build up or accretion of the adhesive on ultrasonic bonding equipment. In one embodiment of the invention, a composite includes an adhesive having a capillary-viscosity value of about 7 Pas·sec or greater and a Shore-OO-Hardness value of about 65 or greater, whereby the relative accretion value is less than about 1, and more particularly less than about 0.5.

Claims (15)

1. A method of making an absorbent product, the method comprising the steps of:

providing a first piece;

providing a second piece; and

attaching at least a portion of the first piece to at least a portion of the second piece using an adhesive composition;

wherein the adhesive composition has a capillary-viscosity value of about 9 Pas·sec or greater and a Shore-OO-Hardness value of about 90 or greater;

exposing at least a part of the composite to ultrasonic energy in a subsequent processing step; and

before, during or after the processing step in which at least a part of the composite is exposed to ultrasonic energy, attaching at least a portion of the composite to at least a portion of a backsheet, a topsheet, or portions of both a backsheet and a topsheet.

2. A method of making an absorbent product, the method comprising the steps of:

providing a first piece;

providing a second piece;

providing at least one elastomeric strand or elastomeric ribbon; and

attaching at least a portion of the strand or ribbon to at least a portion of the first piece and at least a portion of the second piece using an adhesive composition;

wherein the adhesive composition has a capillary-viscosity value of about 9 Pas·sec or greater and a Shore-OO-Hardness value of about 90 or greater, and wherein the creep-resistance value is about 30% or greater;

exposing at least a part of the composite to ultrasonic energy in a subsequent processing step;

and before, during, or after the processing step in which at least a part of the composite is exposed to ultrasonic energy, attaching at least a portion of the composite to at least a portion of a backsheet, a topsheet, or portions of both a backsheet and a topsheet.

Assignments (1)
NAME CHANGE Recorded Feb 3, 2015
From: KIMBERLY-CLARK WORLDWIDE, INC.
To: KIMBERLY-CLARK WORLDWIDE, INC.
Reel/Frame 034880/0742 →