Method for producing flexographic printing plates by means of laser engraving

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,935,236
App. No.
10/380,050
Granted
Aug 30, 2005
Kind
B2
Abstract

The invention relates to a method for producing flexographic printing forms by engraving a printing relief on a flexographic printing element that can be laser engraved, said element having a photochemically cross-linked relief layer. The relief layer is transparent and comprises oxidic, siliceous or zeolitic solid matter with a particle size between 1 and 400 nm in a quantity of between 0.1 and 8 wt. % in relation to the quantity of all components in the relief layer.

Claims (9)

1. A process for the production of flexographic printing plates by laser engraving, comprising the following steps:

(a) application of at least one photochemically crosslinkable relief layer to a dimensionally stable support, where the relief layer comprises at least one elastomeric binder, a polymerizable compound, a photoinitiator or photoinitiator system, a finely divided filler, and a plasticizer

(b) crosslinking of the relief layer over the entire surface by irradiation with actinic light,

(c) engraving of a printing relief into the crosslinked relief layer by means of a laser,

wherein the elastomeric binder is a thermoplastic, elastomeric block copolymer made from alkenylaromatic compounds and 1,3-dienes,

wherein the filler is selected from the group consisting of pyrogenic silicon dioxide, pyrogenic titanium dioxide, pyrogenic aluminum oxide, pyrogenic aluminum-doped silicon dioxide an mixtures thereof having a particle size of from 1 to 400 nm and a specific surface area from 30 to 300 m 2/ g and the amount employed is from 0.2 to 5% by weight, based on the amount of all components of the relief layer,

with the proviso that the relief layer is transparent.

2. A process as claimed in claim 1 , wherein about 1% by weight of the filler is employed.

3. A process as claimed in claim 1 , wherein the elastomeric binder is a styrene-butadiene block copolymer.

Assignments (4)
CHANGE OF NAME Recorded May 15, 2006
From: BASF DRUCKSYSTEME GMBH
To: XSYS PRINT SOLUTIONS DEUTSCHLAND GMBH
Reel/Frame 017626/0132 →
CORRECTIVE ASSIGNMENT TO CORRECT THE ASSIGNEE'S NAMES PREVIOUSLY RECORDED AT REEL 015033 FRAME 0770. Recorded Nov 9, 2004
From: HILLER, MARGIT; SCHADEBRODT, JENS; KACZUN, JUERGEN; NIEDERSTADT, DIETER
To: BASF DRUCKSYSTEME GMBH
Reel/Frame 015967/0392 →
CORRECTIVE ASSIGNMENT TO CORRECT ASSIGNEE'S ADDRESS, PREVIOUSLY RECORDED ON REEL, 014300, FRAME 0062. Recorded Feb 25, 2004
From: HILLER, MARGIT; SCHADEBRODT, JENS; KACZUN, JUERGEN; NIEDERSTADT, DIETER
To: BASF DRUCKERSYSTEME GMBH
Reel/Frame 015033/0770 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 11, 2003
From: HILLER, MARGIT; SCHADERBRODT, JENS; KACZUN, JUERGEN; NIEDERSTADT, DIETER
To: BASF DRUCKSYSTEME GMBH
Reel/Frame 014300/0062 →