Reduction casting method
View Patent ↗A reduction casting method includes the steps of: allowing a metallic gas and a reactive gas to react with each other to generate a reducing compound; introducing the thus-generated reducing compound into a cavity of a molding die 11; and reducing an oxide film formed on a surface of a molten metal by the reducing compound to cast a cast product. The reduction casting method uses a non-reactive gas as a carrier gas when the metallic gas is introduced into the cavity, in which a flow quantity of the non-reactive gas is allowed to be from one sixth to twice that of the reactive gas.
1. A reduction casting method, comprising the steps of:
allowing a metallic gas and a reactive gas to react with each other to generate a reducing compound;
filling the thus-generated reducing compound into a cavity of a molding die; and
casting a cast product while reducing an oxide film formed on a surface of a molten metal by the reducing compound,
wherein a non-reactive gas is used as a carrier gas of the metallic gas,
wherein a flow quantity of the non-reactive gas is set to be from one sixth to twice a flow quantity of the reactive gas.
2. The reduction casting method as set forth in claim 1 , wherein the flow quantity of the non-reactive gas is set to be from one fourth to one half the flow quantity of the reactive gas.
3. The reduction casting method as set forth in claim 1 , wherein the reactive gas is a nitrogen gas, the non-reactive gas is an argon gas and the metallic gas is a magnesium gas.
4. The reduction casting method as set forth in claim 1 , wherein the non-reactive gas is used as the carrier gas when the metallic gas is introduced into the cavity.