Lubricating coating and application process for elastomeric electrical cable accessories
View Patent ↗This invention relates to a method for coating an elastomeric component with a coating that has a low coefficient of friction and the articles formed by the method. The method includes preparing an elastomeric coating; applying the coating to a substrate; contacting the coated substrate with an elastomeric compound; and heating the elastomeric compound and the coated substrate under pressure to bond the coating to the elastomeric compound and form a coated elastomeric component.
1. A method for manufacturing an electrical cable accessory, said method comprising the steps:
providing a substrate having a desired contour in relation to the electrical cable accessory;
coating the substrate with an elastomeric material having a first coefficient of friction and comprising a lubricating constituent to form a coated substrate, wherein the lubricating constituent reduces the first coefficient of friction of the elastomeric material;
contacting the coated substrate with an uncured elastomeric compound having a second coefficient of friction;
curing the elastomeric material and elastomeric compound by applying heat and pressure sufficient to transfer and chemically bond the elastomeric material to the elastomeric compound; and
separating the substrate from the elastomeric material and the elastomeric compound, wherein the elastomeric material coating forms a surface on the elastomeric compound and wherein the reduced first coefficient of friction of the elastomeric material coating is less than the second coefficient of friction of the elastomeric compound.
2. The method for manufacturing an electrical cable accessory according to claim 1 , wherein the elastomeric material is encapsulated with the elastomeric compound or the elastomeric compound is encapsulated by the elastomeric material.
3. The method for manufacturing an electrical cable accessory according to claim 1 , wherein the elastomeric coating comprises a polymer selected from the group consisting of ethylene propylene diene monomer elastomer, ethylene propylene rubber, acrylonitrile-butadiene rubber, natural rubber, butadiene rubber, isoprene rubber, chloro-sulfonyl-polyethylene, vinyl silicone, phenyl methyl vinyl silicone, flouro methyl vinyl silicone and epichlorohydrin rubber.
4. The method for manufacturing an electrical cable accessory according to claim 1 , wherein the lubricating constituent is a powdered material having a coefficient of friction that is less than the coefficient of friction of the elastomeric material.
5. The method for manufacturing an electrical cable accessory according to claim 1 , wherein the elastomeric material is a peroxide curable elastomeric polymer.
6. The method for manufacturing an electrical cable accessory according to claim 1 , wherein the lubricating constituent is selected from the group consisting of polyamides, polyethylene, polypropylene, polyacetal, polytetrafluoroethylene, polydimethylsiloxane, polyester, perfluoropolyether, silicon dioxide, glass microbeads, sand, moylbdenum disulfide, metallic powders, graphite, mica and talc.
7. The method for manufacturing an electrical cable accessory according to claim 1 , wherein the elastomeric coating or the elastomeric compound comprises a peroxide.
8. The method for coating an elastomeric component according to claim 1 , further comprising contacting the coated elastomeric component with a lubricant.
9. The method for coating an elastomeric component according to claim 8 , wherein the lubricant is polydimethylsiloxane (silicone oil), perfluoropolyether, fluorosilicone, phenylmethylpolysiloxane or alkymethylpolysiloxane.
10. The method for coating an elastomeric component according to claim 1 , wherein the coating has a thickness of from about 0.0005-inch thick to 0.020-inch thick.