Cement-containing compositions and method of use

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,033,430
App. No.
10/432,727
Granted
Apr 25, 2006
Kind
B2
Abstract

A settable fluid cementitious composition which is fluid for sufficient time to be suitable for use in a flexible container to provide support in a mine said composition comprises (i) Portland cement in an amount from at least about 8% preferably 10%, (ii) a water soluble silicate in an amount from at least about 2% and (iii) water in an amount to provide a water to solids weight ratio of at lest about 1.2:1 preferably at least abou5 1.5:1 and where the % are by weight based on the combined weights of (i), (ii) and (iii). The viscosity immediately after mixing the components together is sufficiently low that additional water can be incorporated. The composition may include (iv) a pozzolan in an amount from 2 to 35% by weight based on the combined weight of (i), (ii), (iii) and (iv).

Claims (25)

1. A two part settable fluid cementitious composition which is fluid when mixed for sufficient time to be suitable for use in a flexible container to provide support in a mine, said composition comprising:

(i) a first part comprising Portland cement in an amount from at least about 8% and water;

(ii) a second part comprising a water soluble silicate in an amount from at least about 2% and water; and wherein

said water in the first and second parts is present in an amount to provide a water to solids weight ratio of at least about 1.5:1 and wherein the % are by weight based on the combined weights of (i) and (ii).

2. A composition as claimed in claim 1 which exhibits a viscosity immediately after mixing the first and second components together which is sufficiently low that additional water can be incorporated.

3. A composition as claimed in claim 1 , further comprising (iii) a pozzolan in an amount from 2 to 35% by weight based on the combined weight of (i), (ii) and (iii).

4. A composition as claimed in claim 1 wherein the composition has a strength after 2 hours of at least 10 p.s.i.

5. A composition as claimed in claim 1 wherein the composition has a strength after 1 day of at least 50 p.s.i.

6. A composition as claimed in claim 1 wherein the composition has a strength after 7 days of at least 100 p.s.i.

7. A composition as claimed in claim 1 , wherein the Portland cement is present in an amount from at least 10%.

8. A method of providing support in a mine which method comprises providing the two part composition comprised of the first and second components as claimed in claim 1 , pumping the first and second components to a place of use, mixing the first and second components to form a grout, and supplying the grout to a flexible container to inflate the container to provide support in the mine.

9. A method of producing a settable composition which is fluid for sufficient length of time to be suitable for use in a flexible container for providing support in mine, which method comprises:

(i) providing a first component comprising Portland cement, water;

(ii) providing a second component comprising a solution of a silicate in water; and

(iii) mixing the first and second components together to form a settable composition having a minimum solids content of at least 10% by weight and a water to solids weight ratio of at least about 1.5:1.

10. A method as claimed in claim 9 wherein the first component includes a suspension agent to reduce settling out and improve pumpability after standing.

11. A method as claimed in claim 9 wherein the first component includes a retarder for the cement hydration reaction.

12. A system comprising first and second components to be mixed together to form a settable composition, wherein

the first component comprises:

(a) Portland cement;

(b) water, the weight ratio of water to Portland cement being from 0.5:1 to 5:1;

(c) a retarder for the cement hydration reaction; and

(d) a suspension agent, and wherein the second component comprises:

(e) a water soluble silicate; and

(f) water in an amount to provide a weight ratio of water to silicate solids of from 1.5:1 to 25:1.

Assignments (5)
TERMINATION AND RELEASE OF PATENT SECURITY AGREEMENT RECORDED AT REEL 059115, FRAME 0960 Recorded Feb 18, 2025
From: BZ COMMERCIAL FINANCE DESIGNATED ACTIVITY COMPANY
To: MINOVA INTERNATIONAL LIMITED
Reel/Frame 070251/0849 →
SECURITY INTEREST Recorded Feb 28, 2022
From: MINOVA INTERNATIONAL LIMITED
To: BZ COMMERCIAL FINANCE DESIGNATED ACTIVITY COMPANY
Reel/Frame 059115/0960 →
TERMINATION AND RELEASE OF SECURITY INTEREST Recorded Jan 23, 2007
From: BARCLAYS BANK PLC
To: MINOVA INTERNATIONAL LIMITED
Reel/Frame 018787/0674 →
SECURITY AGREEMENT Recorded Apr 4, 2006
From: MINOVA INTERNATIONAL LIMITED (FORMERLY KNOWN AS FOSROC MINING INTERNATIONAL LIMITED)
To: BARCLAYS BANK PLC
Reel/Frame 017411/0822 →
CHANGE OF NAME Recorded Aug 13, 2003
From: FOSROC MINING INTERNATIONAL LIMITED
To: MINOVA INTERNATIONAL LIMITED
Reel/Frame 014379/0229 →