IP Library Granted Patent US 6,921,495
Granted Patent B2
US 6,921,495 · App. 10/479,778 · Granted Jul 26, 2005

Environmentally compatible defrosting and antifreeze agents for aeroplanes

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,921,495
App. No.
10/479,778
Granted
Jul 26, 2005
Kind
B2
Abstract

The invention relates to a deicing or anti-icing composition comprising at least 0.01 to 0.5% wt of at least one alkali metal salt of polyaspartic or polyglutamic acids or a mixture thereof, having a total molecular weight of 5,000 to 50,000 g/mole as a flame retardant. The invention also relates to a method for deicing or preventing the formation of ice on a substrate by applying a composition to the substrate, wherein the composition comprises a flame retardant comprising alkali metal salts of polyaspartic or polyglutamic acids, or a mixture thereof, having a total molecular weight of between 5,000 and 50,000 g/mole, in proportions of 0.01 to 0.5 wt % in relation to the deicing or anti-icing composition. A method of making a deicing or anti-icing composition having a reduced electrochemical activity is also disclosed.

Claims (8)

1. A method for deicing or preventing the formation of ice on a substrate comprising the step of applying a composition to the substrate, wherein the composition comprises a flame retardant, wherein the flame retardant is an alkali metal salt of polyglutamic acid, polyaspartic acid or mixtures thereof, with a molecular weight of from 5000 to 50,000 g/mol, and wherein the flame retardant is present In an amount of from 0.01 to 0.5% by weight, based on the composition.

2. The method as claimed in claim 1 , wherein the flame retardant is present in an amount from 0.02 to 0.5% by weight, based on the weight of the composition.

3. The method as claimed in claim 1 , wherein the molecular weight of the flame retardant is from 8000 to 20,000 g/mol.

4. The method as claimed claim 1 , wherein the composition further comprises at least one glycol present in an amount of from 20 to 97% by weight, wherein the at least one glycol is selected from the group consisting of ethylene glycol, 1,2-propylene glycol, 1,3-propylene glycol, diethylene glycol, dipropylene glycol and mixtures thereof.

5. The method as claimed in claim 1 , wherein the composition further comprises from 0.01 to 1% by weight of at least one anionic and/or nonionic surfactant.

6. A deicing or anti-icing composition comprising a flame retardant, wherein the flame retardant is an alkali metal salt of polyglutamic acid, polyaspartic acid or mixtures thereof, with a molecular weight of from 5000 to 50,000 g/mol, and wherein the flame retardant is present in an amount of from 0.01 to 0.5% by weight, based on the composition.

7. A method of making a deicing or anti-icing composition having a reduced electrochemical activity, said method comprising the step of adding a flame retardant to the composition, wherein the flame retardant is an alkali metal salt of polyglutamic acid, polyaspartic acid or mixtures thereof, with a molecular weight of from 5000 to 50,000 g/mol, and where in the flame retardant is present in an amount of from 0.01 to 0.5% by weight, based on the composition.

8. The method of claim 7 , wherein the amount of flame retardant added provides an electrochemical activity of less than 25 mA as measured at 20° C. between 2 silver-coated copper conductors carrying a direct current of 28 volts.