IP Library Granted Patent US 6,936,216
Granted Patent B2
US 6,936,216 · App. 10/492,988 · Granted Aug 30, 2005

Melt launder

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,936,216
App. No.
10/492,988
Granted
Aug 30, 2005
Kind
B2
Abstract

The invention relates to a melt launder ( 1, 9, 10 ) comprising a bottom and edged, said melt launder being particularly meant to be used for tapping a molten phase, such as slag, from a smelting furnace, which melt launder is manufactured of copper or copper alloy and provided with cooling channels ( 8 ), so that at the bottom ( 2 ) of the melt launder ( 1, 9, 10 ), there is arranged at least one groove ( 3 ).

Claims (11)

1. A melt launder for tapping a molten phase from a smelting furnace, the melt launder comprising:

a bottom portion and edge portions, made of copper or copper alloy, for contacting the molten phase, the edge portions being provided with cooling channels situated in a lengthwise direction of the melt launder, above a level the molten phase reaches during use, the bottom portion of the melt launder having at least one groove adapted to hold a fire-resistant material that contacts the molten phase during use.

2. A melt launder according to claim 1 , wherein the bottom portion has at least one lengthwise groove and at least one transverse groove extending a width of the melt launder.

3. A melt launder according to claim 1 , further comprising a fire-resistant material situated in the at least one groove.

4. A melt launder according to claim 3 , wherein the fire-resistant material is a material that is capable of being autogenously replaced by solidified melt.

5. A melt launder according to claim 1 , wherein the at least one groove is 5-25 mm deep and 5-25 mm wide.

6. A melt launder according to claim 1 , wherein a plurality of grooves are provided, each groove being separated from an adjacent groove by a distance of 5-25 mm.

7. A melt launder according to claim 1 , wherein the at least one groove is located a distance of at least 30 mm from a lowermost cooling channel.

8. A melt launder according to claim 1 , wherein the bottom portion and edge portions of the melt launder are manufactured from a single bent copper element.

9. A melt launder according to claim 1 , wherein the bottom portion and edge portions of the melt launder are manufactured from two straight copper plates, which are worked into a substantially V-shape.

10. A melt launder according to claim 1 , wherein the bottom portion and edge portions of the melt launder consist of separate parts.

Assignments (3)
CHANGE OF NAME Recorded Jul 22, 2013
From: OUTOKUMPU TECHNOLOGY OY
To: OUTOTEC OYJ
Reel/Frame 030851/0419 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 11, 2005
From: OUTOKUMPU OYJ
To: OUTOKUMPU TECHNOLOGY OY
Reel/Frame 016497/0028 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 16, 2004
From: KOJO, ILKKA; JOKILAAKSO, ARI
To: OUTOKUMPU OYJ
Reel/Frame 015673/0651 →