IP Library Granted Patent US 7,955,539
Granted Patent B2
US 7,955,539 · App. 10/507,230 · Granted Jun 7, 2011

Reversible, heat-set, elastic fibers, and method of making and article made from same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,955,539
App. No.
10/507,230
Granted
Jun 7, 2011
Kind
B2
Abstract

A reversible, heat-set covered fiber is described, the covered fiber comprising: A. A core comprising an elastic fiber comprising a substantially crosslinked, temperature-stable, olefin polymer, and B. A cover comprising an inelastic fiber. The fiber is heat-set by a method comprising: (a) Stretching the covered fiber by applying a stretching force to the covered fiber; (b) Heating the stretched covered fiber of (a) to a temperature in excess of the crystalline melting point of the olefin polymer for a period of time sufficient to at least partially melt the olefin polymer; (c) Cooling the stretched and heated covered fiber of (b) to a temperature below the crystalline melting point of the olefin polymer for a period of time sufficient to solidify the polymer; and (d) Removing the stretching force from the covered fiber.

Claims (7)

1. A method of making a reversed, heat-set elastic fiber comprising:

(a) applying a biasing force to an elastic fiber that will recover at least 50% of its stretched length after the first pull and after the fourth pull of four consecutive pulls to 100% strain, wherein the elastic fiber is a melt spun elastic fiber;

(b) heating the stretched fiber of (a) to a temperature in excess of a temperature at which at least a portion of the crystallites are molten;

(c) cooling the fiber of (b) to a temperature below the temperature of step (b);

(d) removing the biasing force from the fiber; and thereafter

(e) heating the temperature of the fiber above a temperature at which at least a portion of the crystallites are molten without a biasing force, such that the length of the fiber obtained in step (e) is less than the length of the fiber obtained in step (d).

2. The method of claim 1 wherein the elastic fiber is fiber is combined with inelastic fiber to form a yarn prior to step (a).