Removal of blockages from pipework using carbamate and nitric acid treatment steps

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,047,985
App. No.
10/510,248
Granted
May 23, 2006
Kind
B2
Abstract

The invention provides a method for the removal of contaminating materials from pipework, the contaminating materials comprising deposits on the pipework which cause a reduction in the effective internal diameter of the pipes and thereby effect a reduction in the rate of flow of a fluid through the pipework, the method comprising treating the contaminating materials with at least one carbamate salt. The methods is also suitable for the treatment of contaminating materials which have a particularly deleterious effect on fluid flow and comprise partial or total blockages of the pipework. The carbamate is preferably in the form of an aqueous solution, and a preferred carbamate salt is ammonium carbamate. The treatment may be carried out in the presence of an additive such as caesium carbonate or ammonium bicarbonate. Optionally the treatment may be accompanied by a pre-treatment or post-treatment with aid, this being followed by a water wash. The method finds particular application in the nuclear processing industry.

Claims (24)

1. A method for the removal of contaminating materials from pipework in the nuclear processing industry, said contaminating materials comprising deposits on the pipework which comprise inorganic salts having low solubility levels, wherein said contaminating materials cause a reduction in the effective internal diameter of the pipes and thereby effect a reduction in the rate of flow of a fluid through the pipework, the method comprising treating pipework used in the nuclear processing industry for the processing of Highly Active Liquor as follows:

(a) treating with 2.0M nitric acid at room temperature; followed by

(b) washing with water at room temperature; followed by

(c) treating with 1.0M or 3.0M aqueous ammonium carbamate solution at 60° C. for 2 hours.

2. The method of claim 1 wherein said inorganic salts are deposited from solutions or suspensions in contact with the pipework.

3. The method of claim 1 wherein said inorganic salts comprise phosphate, alkylphosphate, molybdate and phosphomolybdate salts.

4. The method of claim 3 wherein said salts comprise the phosphate, butylphosphate, molybdate and phosphomolybdate salts of zirconium, tellurium, gadolinium, caesium, iron and uranium.

5. The method of claim 1 wherein said contaminating materials result in the partial or total blockage of the pipework.

6. The method of claim 1 wherein said treatment is carried out in the presence of at least one additive.

7. The method of claim 6 wherein said additive comprises a carbonate or bicarbonate salt.

8. The method of claim 7 wherein said carbonate or bicarbonate salt comprises caesium carbonate or ammonium bicarbonate.

9. The method of claim 1 comprising the treatment of pipework used in the processing of Highly Active Liquor with an aqueous solution comprising 1.0M ammonium carbamate and further comprising 0.2M caesium carbonate at 60° C. for 2 hours.

10. A method for the removal of contaminating materials from pipework in the nuclear processing industry, said contaminating materials comprising deposits on the pipework which comprise inorganic salts having low solubility levels, wherein said contaminating materials cause a reduction in the effective internal diameter of the pipes and thereby effect a reduction in the rate of flow of a fluid through the pipework, the method comprising treating pipework used in the nuclear processing industry for the processing of Highly Active Liquor as follows:

(a) treating with 1.0M or 3.0M aqueous ammonium carbamate solution at 60° C. for 2 hours; followed by

(b) treating with 2.0M nitric acid at room temperature; followed by

(c) washing with water at room temperature.

11. The method of claim 10 wherein said inorganic salts are deposited from solutions or suspensions in contact with the pipework.

12. The method of claim 10 wherein said inorganic salts comprise phosphate, alkylphosphate, molybdate and phosphomolybdate salts.

13. The method of claim 12 wherein said salts comprise the phosphate, butylphosphate, molybdate and phosphomolybdate salts of zirconium, tellurium, gadolinium, caesium, iron and uranium.

14. The method of claim 10 wherein said contaminating materials result in the partial or total blockage of the pipework.

15. The method of claim 10 wherein said treatment is carried out in the presence of at least one additive.

16. The method of claim 15 wherein said additive comprises a carbonate or bicarbonate salt.

17. The method of claim 16 wherein said carbonate or bicarbonate salt comprises caesium carbonate or ammonium bicarbonate.

18. The method of claim 10 comprising treatment pipework used in the processing of Highly Active Liquor with an aqueous solution comprising 1.0M ammonium carbamate and further comprising 0.2M caesium carbonate at 60° C. for 2 hours.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 8, 2008
From: BRITISH NUCLEAR FUELS PLC
To: NUCLEAR DECOMMISSIONING AUTHORITY
Reel/Frame 020482/0750 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 12, 2005
From: DENNIS, IAN STEWART; MAYHEW, PHILLIP ANTONY
To: BRITISH NUCLEAR FUELS PLC
Reel/Frame 016250/0727 →