Collecting agent for sulphidic ores, the production and use thereof
View Patent ↗A method for the flotation of sulfide ores is disclosed. The method comprises contacting the sulfide ores with a composition comprising at least one compound of the formula where R 1 , R 2 and R 3 independently of one another are alkyl groups having 1 to 18 carbon atoms, alkenyl groups having 2 to 18 carbon atoms, aryl groups having 6 to 10 carbon atoms, or alkylaryl groups having 7 to 10 carbon atoms.
1. A method for flotation of sulfide ores, said method comprising contacting said sulfide ores with at least one compound of the formula
where R 1, R 2 and R 3 independently of one another are alkyl groups having 1 to 18 carbon atoms, alkenyl groups having 2 to 18 carbon atoms, aryl groups having 6 to 10 carbon atoms, or alkylaryl groups having 7 to 10 carbon atoms, and R 4 is hydrogen or alkyl groups having 1 to 18 carbon atoms, alkenyl groups having 2 to 18 carbon atoms, aryl groups having 6 to 10 carbon atoms, or alkylaryl groups having 7 to 10 carbon atoms and subjecting the contacted sulfide ore to flotation.
2. The method of claim 1 , wherein R 1, R 2 and R 3 independently of one another are C 2 –C 4 -alkyl groups.
3. The method of claim 1 , wherein said contacting occurs in a pH range from 2 to 12.
4. The method of claim 1 , wherein the compound is present in amounts of 0.001 to 1.0 kg per tonne of said ores.
5. The method of claim 1 , wherein said sulfide ores are nonferrous sulfide ores, the nonferrous sulfide ores selected from the group consisting of copper sulfide, nickel sulfide, zinc sulfide, lead sulfide, molybdenum sulfide, and mixtures thereof.