Grafting polymerization of guar and other polysaccharides by electron beams

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,838,667
App. No.
10/607,079
Granted
Nov 23, 2010
Kind
B2
Abstract

A method of grafting galactomannan-type polysaccharide polymers, preferably guar, to a functional group by irradiation with high energy electron beams in the presence of an unsaturated monomer-compressing the described functional group. The method may include the depolymerization of the grafted polymer to a pre-selected low molecular weight. The preferred galactomannans for treatment according to this method are guar gum, guar splits and hydroxypropyl guar. In a preferred embodiment the guar gum is also depolymerized, preferably to a molecular weight of below about 700,000 Daltons, and most preferably to a molecular weight of between about 100,000 Daltons to about 250,000 Daltons. The depolymerized guar most preferably has a polydispersity of less than about 3.0 and is useful in oil well fracturing to enhance oil production.

Claims (10)

1. A method for grafting an unsaturated monomer onto a guar comprising the steps of: (1) forming a mixture comprised of an unsaturated monomer having a functional group selected from quaternary ammonium and a water-soluble or water-dispersible guar; (2) drying the mixture and (3) irradiating the mixture with an amount of electron beam radiation sufficient to form an unsaturated monomer-water-soluble or water-dispersible guar graft copolymer, wherein the graft copolymer is depolymerized to a molecular weight lower than the molecular weight of the ungrafted guar, and the guar in the copolymer has a molecular weight of between 100,000 and 700,000 Daltons.

2. The method of claim 1 , wherein the unsaturated monomer is a vinyl monomer having a quaternary ammonium group selected from methacrylamidopropyltrimethylammonium chloride.

3. The method of claim 1 , wherein the guar is selected from the group consisting of guar gum and guar powder.

4. The method of claim 3 , wherein the unsaturated monomer is a vinyl monomer having a quaternary ammonium group selected from methacrylamidopropyltrimethylammonium chloride.

5. The method of claim 1 , wherein the guar is guar powder.

6. The method of claim 5 , wherein the unsaturated monomer is a vinyl monomer having a quaternary ammonium group selected from methacrylamidopropyltrimethylammonium chloride.

7. The method of claim 1 , wherein the guar is guar gum.

8. The method of claim 5 , wherein the unsaturated monomer is a vinyl monomer having a quaternary ammonium group selected from methacrylamidopropyltrimethylammonium chloride.

9. A method for grafting an unsaturated monomer onto a guar comprising the steps of: (1) forming a mixture comprised of an unsaturated monomer having a functional group selected from quaternary ammonium and a water-soluble or water-dispersible guar; (2) drying the mixture in the air and (3) irradiating the mixture with an amount of electron beam radiation sufficient to form an unsaturated monomer-water-soluble or water-dispersible guar graft copolymer, wherein the graft copolymer is depolymerized to a molecular weight lower than the molecular weight of the ungrafted guar, and the guar in the copolymer has a molecular weight of between 100,000 and 700,000 Daltons.

10. A method for grafting an unsaturated monomer onto a guar comprising the steps of: (1) forming a mixture comprised of an unsaturated monomer having a functional group selected from quaternary ammonium and a water-soluble or water-dispersible guar; (2) drying the mixture in a vacuum and (3) irradiating the mixture with an amount of electron beam radiation sufficient to form an unsaturated monomer-water-soluble or water-dispersible guar graft copolymer, wherein the graft copolymer is depolymerized to a molecular weight lower than the molecular weight of the ungrafted guar, and the guar in the copolymer has a molecular weight of between 100,000 and 700,000 Daltons.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 3, 2011
From: RHODIA INC.
To: RHODIA OPERATIONS
Reel/Frame 025756/0342 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 20, 2011
From: RHODIA INC.
To: RHODIA OPERATIONS
Reel/Frame 025736/0801 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 23, 2005
From: LIU, LEO ZHAOQING; PRIOU, CHRISTIAN
To: RHODIA INC.
Reel/Frame 015768/0438 →