IP Library Granted Patent US 7,009,005
Granted Patent B2
US 7,009,005 · App. 10/694,800 · Granted Mar 7, 2006

Thin-layer-covered golf ball with improved velocity

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,009,005
App. No.
10/694,800
Granted
Mar 7, 2006
Kind
B2
Abstract

A golf ball comprising a center comprising a polybutadiene having a molecular weight of greater than 200,000 and a resilience index of at least about 40; and a cover layer comprising a polyurethane composition formed from a prepolymer having no greater than 7.5 percent by weight unreacted isocyanate groups.

Claims (39)

1. A golf ball comprising:

a center formed of a reaction product having a dynamic stiffness of less than about 50,000 N/m at −50°C. comprising:

polybutadiene having a molecular weight of greater than about 200,000;

a crosslinking material present in an amount of about 10 to about 40 parts per hundred of the reaction product;

a free radical source present in an amount of about 0.1 to about 15 parts per hundred of the reaction product;

a cis-to-trans catalyst present in an amount of about 0.1 to about 10 parts per hundred of the reaction product, wherein the cis-to-trans catalyst comprises a metal organosulfur compound; and

a cover comprising a thermoplastic or thermoset polyurethane.

2. The golf ball of claim 1 , wherein the dynamic stiffness is about 10,000 N/m to about 40,000 N/m at −50° C.

3. The golf ball of claim 2 , wherein the dynamic stiffness is about 20,000 N/m to about 30,000 N/m at −50° C.

4. The golf ball of claim 1 , wherein the molecular weight of the polybutadiene is greater than about 250,000.

5. The golf ball of claim 4 , wherein the molecular weight of the polybutadiene is from about 300,000 to about 500,000.

6. A golf ball comprising:

a center formed of a reaction product comprising:

polybutadiene having a molecular weight of greater than about 200,000;

a crosslinking material present in an amount of about 10 to about 40 parts per hundred of the reaction product;

a free radical source present in an amount of about 0.1 to about 15 parts per hundred of the reaction product;

a cis-to-trans catalyst present in an amount of about 0.1 to about 10 parts per hundred of the reaction product, wherein the reaction product has a percent change in dynamic stiffness from 0° C. to −50° C. of less than 20 percent, wherein the cis-to-trans catalyst comprises a metal organosulfur compound; and

a cover comprising a thermoplastic or thermoset polyurethane.

7. The golf ball of claim 6 , wherein the molecular weight of the polybutadiene is about 250,000 or greater.

8. The golf ball of claim 7 , wherein the molecular weight of the polybutadiene is about 300,000 to about 500,000.

9. The golf ball of claim 6 , wherein the crosslinking material is present in an amount of about 10 to about 30 parts per hundred of the reaction product.

10. The golf ball of claim 6 , wherein the free radical comprise a peroxide present in an amount of about 0.2 to about 5 parts per hundred of the reaction product.

11. The golf ball of claim 6 , wherein the cis-to-trans catalyst is present in an amount of about 0.1 to about 8 parts per hundred of the reaction product.

12. A golf ball comprising:

a center formed of a reaction product having a dynamic stiffness of less than about 50,000 N/m at −50° C. and a percent change in dynamic stiffness from 0°C. to −50° C. of less than 20 percent, wherein the reaction product comprises:

polybutadiene having a molecular weight of greater than about 200,000;

a crosslinking material present in an amount of about 10 to about 40 parts per hundred of the reaction product;

a free radical source present in an amount of about 0.1 to about 15 parts per hundred of the reaction product;

a cis-to-trans catalyst present in an amount sufficient to produce a reaction product having at least 32 percent trans-isomer; and

a cover comprising a castable reactive liquid material.

13. The golf ball of claim 12 , wherein the dynamic stiffness is about 10,000 N/m to about 40,000 N/m at −50° C.

14. The golf ball of claim 13 , wherein the dynamic stiffness is about 20,000 N/m to about 30,000 N/m at −500° C.

15. The golf ball of claim 12 , wherein the castable reactive liquid material comprises polyurethane.

16. The golf ball of claim 12 , wherein the cis-to-trans catalyst comprises at least one of an organosulfur compound, an aromatic organic compound, or a mixture thereof.

17. The golf ball of claim 16 , wherein the organosulfur compound comprises metal.

18. The golf ball of claim 16 , wherein the organosulfur compound comprises less than about 3 weight percent metal.

19. The golf ball of claim 18 , wherein the organosulfur compound comprises less than about 0.01 weight percent metal.

20. The golf ball of claim 16 , wherein the aromatic organic compound is substantially free of metal.

21. The golf ball of claim 16 , wherein the aromatic organic compound comprises a hydroxy group, a metal salt of a hydroxyl, a mercapto group, a metal salt of a mercapto group, a carboxy group, a metal salt of a carboxyl, an acrylate, a metal salt an acrylate, or a combination thereof.

Assignments (5)
ASSIGNMENT OF SECURITY INTEREST IN PATENTS (ASSIGNS 039506-0030) Recorded Aug 3, 2022
From: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS RESIGNING ADMINISTRATIVE AGENT
To: JPMORGAN CHASE BANK, N.A., AS SUCCESSOR ADMINISTRATIVE AGENT
Reel/Frame 061521/0414 →
RELEASE OF SECURITY INTEREST IN PATENTS PREVIOUSLY RECORDED AT REEL/FRAME (027332/0366) Recorded Sep 7, 2016
From: KOREA DEVELOPMENT BANK, NEW YORK BRANCH
To: ACUSHNET COMPANY
Reel/Frame 039938/0979 →
SECURITY INTEREST Recorded Jul 28, 2016
From: ACUSHNET COMPANY
To: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS ADMINISTRATIVE AGENT
Reel/Frame 039506/0030 →
SECURITY AGREEMENT Recorded Dec 7, 2011
From: ACUSHNET COMPANY
To: KOREA DEVELOPMENT BANK, NEW YORK BRANCH
Reel/Frame 027332/0366 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 29, 2003
From: WU, SHENSHEN; HEBERT, EDMUND A.; BISSONNETTE, LAURENT C.; BULPETT, DAVID A.; RAJAGOPALAN, MURALI; VOORHEIS, PETER; WRIGLEY, MARK N.
To: ACUSHNET COMPANY
Reel/Frame 014671/0107 →