IP Library Granted Patent US 7,216,512
Granted Patent B2
US 7,216,512 · App. 10/698,220 · Granted May 15, 2007

Method of making an optical fiber by laser cleaving

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,216,512
App. No.
10/698,220
Granted
May 15, 2007
Kind
B2
Abstract

A field-installable connector includes a connector housing and a ferrule having front and rear opposed faces and at least one fiber bore defined longitudinally therethrough. A laser processed stub optical fiber is disposed within the one fiber bore of the ferrule and extends a predetermined distance beyond the rear face of the ferrule. An alignment feature is operable for self-centering the stub optical fiber and a field optical fiber to perform a mechanical splice using a camming means. A method of laser processing a stub optical fiber includes rotating the stub optical fiber and sweeping a laser beam directed at a desired angle back and forth across a surface of the optical fiber. An oscillating motion of the laser is driven by an intermittent sinusoidal signal that results in two deposits of energy onto the stub optical fiber followed by a cooling period before subsequent deposits of energy occur.

Claims (21)

1. A method of fabricating a field-installable connector adapted to be mechanically spliced to a field optical fiber, comprising:

rotating a stub optical fiber secured within a ferrule of the field-installable connector; and

laser processing the stub optical fiber to create an endface by sweeping a laser beam directed at a preselected angle from perpendicular to a longitudinal axis of the stub optical fiber back and forth across a surface of the rotating stub optical fiber.

2. The method of claim 1 ;

wherein an oscillating motion of the laser is driven by an intermittent sinusoidal signal resulting in at least one deposit of energy onto the stub optical fiber followed by a cooling period before a subsequent deposit of energy occurs; and

wherein a pulse duration and a laser energy are predetermined so that the stub optical fiber is progressively ablated without re-depositing ablated material or distorting the geometry of the remaining stub optical fiber.

3. The method of claim 1 , wherein the preselected angle ranges from about 10° to about 60° from pependicularto the longitudinal axis of the stub optical fiber.

4. The method of claim 1 , wherein the preselected angle ranges from about 25° to about 35° from perpendicular to the longitudinal axis of the stub optical fiber.

5. The method of claim 1 , wherein the laser is focused to a spot size that is slightly larger than the diameter of the stub optical fiber.

6. The method of claim 1 , wherein the stub optical fiber is positioned from about 2 to about 2.5 fiber widths downward from an uppermost peak of a sinusoidal laser path and about 8 to about 10 fiber widths upward from a dwell position of the laser.

7. The method of claim 1 , wherein the step of laser processing the stub optical fiber is achieved by impinging an amount of laser energy at a preselected laser intensity in the form of a Gaussian intensity distribution onto the stub optical fiber.

8. The method of claim 1 , wherein the step of laser processing the stub optical fiber creates a dome shaped endface having a protruding fiber core.

9. A method of laser processing an optical fiber, comprising;

rotating the optical fiber; and

sweeping a beam of a laser directed at a preselected angle from perpendicular to a longitudinal axis of the optical fiber back and forth across a surface of the rotating optical fiber;

wherein the laser is operated in a continuous mode;

wherein an oscillating motion of the laser is driven by an intermitting sinusoidal signal resulting in two deposits of energy onto the optical fiber followed by a cooling period before subsequent deposits of energy occur; and

wherein a pulse duration and an energy intensity of the laser are preselected so that the optical fiber is progressively ablated without re-depositing ablated material or distorting the geometry of the remaining optical fiber.

10. The method of claim 9 , wherein the preselected angle ranges from about 10° to about 60°.

11. The method of claim 9 , wherein the preselected angle ranges from about 25° to about 35°.

12. The method of claim 9 , wherein the step of sweeping a laser creates a dome shaped endface having a protruding fiber core on the optical fiber.

Assignments (2)
MERGER Recorded Aug 18, 2017
From: CCS TECHNOLOGY, INC.; CORNING OPTICAL COMMUNICATIONS BRANDS, INC.
To: CORNING OPTICAL COMMUNICATIONS LLC
Reel/Frame 043601/0427 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 25, 2014
From: CORNING CABLE SYSTEMS LLC
To: CCS TECHNOLOGY, INC.
Reel/Frame 033601/0127 →