IP Library Granted Patent US 7,776,454
Granted Patent B2
US 7,776,454 · App. 10/743,641 · Granted Aug 17, 2010

Ti brazing strips or foils

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,776,454
App. No.
10/743,641
Granted
Aug 17, 2010
Kind
B2
Abstract

A method for producing titanium alloy brazing strips and the resulting brazing strips and/or foils. The method uses a cold-rolling process without heat treating to generate a titanium based multi-layer alloy strip or foil made up of discrete layers of titanium and an additional layer or layers of one or more metals, such as zirconium, nickel and/or copper, for example, or alloys thereof, with the layer of titanium roll bonded without heat treating to the layers of the additional metal(s). The resulting strip or foil can include, for example, Cu/Ti/Cu, Ni/Ti/Ni, Ni/Ti/Cu, Cu/Ni/Ti/Ni/Cu, Ni/Cu/Ti/Cu/Ni, Ni/Cu/Ni/Ti/Ni/Cu/Ni, Ni/Zr/Cu/Ti/Cu/Zr/Ni and Ni/Ti/Cu/Zr/Cu/Ti/Ni among other combinations. The resulting strip or foil can be used for brazing, creating an alloy of the weight percentage of the original materials.

Claims (32)

1. A brazing strip or foil comprising:

a first layer including one or both of nickel and copper;

a second layer including one or both of ‘titanium and zirconium;

a third layer including one or both of nickel and copper; a fourth layer including one or both of nickel and copper;

a fifth layer including one or both of titanium and zirconium; a sixth layer including one or both of nickel and copper, and

a core including one of titanium and zirconium, wherein said core is in a middle of said layers, wherein the weight percentage of the resulting brazing strip or foil results in about a 20Cu-20Ni-20Zr-40Ti alloy upon brazing.

2. A brazing strip or foil comprising:

a first layer including one or both of nickel and copper;

a second layer including one or both of ‘titanium and zirconium;

a third layer including one or both of nickel and copper; a fourth layer including one or both of nickel and copper;

a fifth layer including one or both of titanium and zirconium; a sixth layer including one or both of nickel and copper, and

a core including one of titanium and zirconium, wherein said core is in a middle of said layers wherein the weight percentage of the resulting brazing strip or foil results in about a 15Cu-10Ni-37Zr-38Ti alloy upon brazing.

3. A brazing strip or foil comprising:

a first layer including one or both of nickel and copper;

a second layer including zirconium;

a third layer including one or both of nickel and copper;

a fourth layer including one or both of nickel and copper;

a fifth layer including zirconium;

a sixth layer including one or both of nickel and copper, and a core layer including titanium layered in the center of said strip or foil, wherein

said second layer has a metallic bond with both said first and said third layers, and wherein

said core layer has a metallic bond with both said third and said fourth layers, and further wherein

said fifth layer has a metallic bond with both said fourth and said sixth layers wherein the metallic bond is formed by roll-bonding without any heat treatment wherein the weight percentage of the resulting brazing strip or foil results in about a 20Cu-20Ni-20Zr-40Ti alloy upon brazing.

4. A brazing strip or foil comprising:

a first layer including one or both of nickel and copper;

a second layer including zirconium;

a third layer including one or both of nickel and copper;

a fourth layer including one or both of nickel and copper;

a fifth layer including zirconium;

a sixth layer including one or both of nickel and copper, and a core layer including titanium layered in the center of said strip or foil, wherein

said second layer has a metallic bond with both said first and said third layers, and wherein

said core layer has a metallic bond with both said third and said fourth layers, and further wherein

said fifth layer has a metallic bond with both said fourth and said sixth layers wherein the metallic bond is formed by roll-bonding without any heat treatment wherein the weight percentage of the resulting brazing strip or foil results in about a 15Cu-10Ni-37Zr-38Ti alloy upon brazing.

Assignments (3)
TERMINATION AND RELEASE OF GRANT OF SECURITY INTEREST IN PATENTS Recorded Oct 23, 2017
From: U.S. BANK NATIONAL ASSOCIATION
To: EMS ENGINEERED MATERIALS SOLUTIONS, LLC
Reel/Frame 044259/0546 →
SECURITY INTEREST Recorded Oct 23, 2017
From: EMS ENGINEERED MATERIALS SOLUTIONS, LLC
To: WELLS FARGO BANK, NATIONAL ASSOCIATION
Reel/Frame 043919/0722 →
SECURITY AGREEMENT Recorded Sep 5, 2013
From: ICON AGENT, LLC
To: EMS ENGINEERED MATERIALS SOLUTIONS, LLC
Reel/Frame 031170/0965 →