IP Library Granted Patent US 7,183,343
Granted Patent B2
US 7,183,343 · App. 10/782,753 · Granted Feb 27, 2007

Thermoplastic vulcanizate with improved surface properties

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,183,343
App. No.
10/782,753
Granted
Feb 27, 2007
Kind
B2
Abstract

The invention concerns a thermoplastic vulcanizate, comprising the following components: a thermoplastic (A); an at least partially vulcanized rubber (B); a plasticizer (C); conventional additives (D); and a surface modifier (E), which migrates uniformly onto the surface of the vulcanizate and forms a continuous, waxlike, solid layer.

Claims (16)

1. A thermoplastic vulcanizate, comprising:

a thermoplastic (A);

an at least partially vulcanized rubber (B);

a plasticizer (C);

conventional additives (D) other than plasticizer or surface modifier; and

a surface modifier (E) containing hydrogenated castor oil, which migrates uniformly onto a surface and forms a wax layer.

2. The thermoplastic vulcanizate according to claim 1 , wherein conventional additives are selected from the group consisting of fillers, aging protectants, UV stabilizers, UV absorbers, color pigments, flameproofing agents, flow promoters and process adjuvants.

3. The thermoplastic vulcanizate according to claim 1 , wherein the vulcanizate has the following quantitative portions in regard to components (A, B, C):

thermoplastic rubber (A)

 60 to 5 wt. %

rubber (B)

20 to 45 wt. %

plasticizer (C)

20 to 50 wt. %.

4. The thermoplastic vulcanizate according to claim 3 wherein the conventional additives (D) are added in 0.02 to 0.5-fold weight amount, in reference to the total of the three components (A, B, C).

5. The thermoplastic vulcanizate according to claim 4 wherein the surface modifier (B) is added in 0.005 to 0.1-fold weight amount, in reference to the total of the four components (A, B, C, D).

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Feb 23, 2007
From: U.S. BANK TRUST NATIONAL ASSOCIATION; PATRICK J. CROWLEY, TRUSTEE
To: POLYONE CORPORATION
Reel/Frame 018923/0081 →
SECURITY INTEREST Recorded Jan 17, 2005
From: POLYONE CORPORATION
To: U.S. BANK TRUST NATIONAL ASSOCIATION; ANGELITA PENA, INDIVIDUAL TRUSTEE, C/O U.S. BANK TRUST NATIONAL ASSOCIATION
Reel/Frame 015599/0598 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 3, 2004
From: VORTKORT, JORG
To: POLYONE CORPORATION
Reel/Frame 014688/0389 →