Method of making an electrode for a membrane electrode assembly and method of making the membrane electrode assembly

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,153,802
App. No.
10/820,639
Granted
Dec 26, 2006
Kind
B2
Abstract

A method of making an electrode decal, comprises forming a catalyst ink comprising a catalyst compound, a perfluorinated sulfonyl fluoride polymer, and an ester; disposing the catalyst ink on a decal; and drying the catalyst ink to form an electrode layer on the decal.

Claims (12)

1. A method of making an electrode layer, comprising:

forming a catalyst ink comprising a catalyst compound, a perfluorinated sulfonyl fluoride polymer, and an ester, wherein in the ink comprises about 20 wt % to about 30 wt % of the catalyst compound, about 15 wt % to about 20 wt % the ester, about 40 wt % to about 50 wt % perfluorinated sulfonyl fluoride polymer, and about 5 wt % to about 10 wt % polyvinyl alcohol, wherein the weight percentages are based on the total weight of the ink;

disposing the catalyst ink on substrate; and

drying the catalyst ink to form the electrode layer on the substrate.

2. The method of claim 1 wherein the ester is synthesized from acetic acid.

3. The method of claim 2 wherein the ester is n-propyl acetate.

4. The method of claim 1 , wherein the catalyst compound comprises platinum and the ester is n-propyl acetate.

5. The method of claim 1 , wherein the catalyst compound is selected from the group consisting of platinum, palladium, rhodium, carbon, gold, tantalum, tungsten, ruthenium, iridium, osmium, and an alloy and combination comprising at least one of the foregoing catalyst compounds.

6. The method of claim 1 wherein the catalyst compound has a particle size of about 10 nanometers to about 100 nanometers.

7. The method of claim 1 , wherein the electrode layer has a thickness of less than or equal to about 2 micrometers.

8. The method of claim 1 , wherein the substrate is a decal.

9. The method of claim 1 , wherein the substrate is a proton exchange membrane.

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Feb 19, 2013
From: PERSEUS PARTNERS VII, L.P.
To: PROTON ENERGY SYSTEMS, INC.
Reel/Frame 029834/0750 →
SECURITY AGREEMENT Recorded Jun 8, 2007
From: PROTON ENERGY SYSTEMS, INC.
To: PERSEUS PARTNERS VII, L.P.
Reel/Frame 019399/0436 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 21, 2004
From: MANCO, JUDITH; CAPUANO, CHRISTOPHER; NAVA, JUAN; TINOCO, FLAVIO
To: PROTON ENERGY SYSTEMS, INC.
Reel/Frame 015590/0049 →