IP Library Granted Patent US 7,943,070
Granted Patent B1
US 7,943,070 · App. 10/839,639 · Granted May 17, 2011

Molded thin-layer lignocellulose composites having reduced thickness and methods of making same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,943,070
App. No.
10/839,639
Filed
May 5, 2004
Granted
May 17, 2011
Kind
B1
Art Unit
1786
USPC
264/120
Abstract

Thin-layer lignocellulose composites having reduced thickness and methods for the manufacture of such thin-layer composites are disclosed. Also described is a process for making wood-based composite door skins of reduced thickness. The door skins may be less than 0.115 inches (2.92 mm) thick.

Claims (44)

1. A method for making a molded thin-layer composite of reduced thickness comprising the steps of:

forming a mixture comprising a refined lignocellulosic fiber, a resin, and a wax selected from the group consisting of paraffin wax, microcrystalline wax, shellac wax, ozokerite wax, montan wax, slack wax, emulsified waxes thereof, and combinations thereof;

pre-pressing the mixture into a loose mat;

coating at least one of two dies with an anti-bonding agent including a ceramic layer; and

pressing the mat between the two dies at an elevated temperature and pressure and for sufficient time to form a thin-layer lignocellulosic composite comprising a thickness from about 0.063 inches (1.60 mm) to 0.115 inches (2.92 mm).

2. The method of claim 1 , wherein the resin comprises a formaldehyde-based resin or an isocyanate-based resin.

3. The method of claim 1 , wherein the mixture comprises an internal release agent that is an aqueous emulsion of surfactants and polymers distinct from the wax.

4. A method for making a door skin of reduced thickness comprising the steps of:

forming a mixture comprising a refined lignocellulosic fiber, a resin, and a wax selected from the group consisting of paraffin wax, microcrystalline wax, shellac wax, ozokerite wax, montan wax, slack wax, emulsified waxes thereof, and combinations thereof;

pre-pressing the mixture into a loose mat;

coating at least one of two dies with an anti-bonding agent including a ceramic layer; and

pressing the mat between the two dies at an elevated temperature and pressure and for sufficient time to form a thin-layer lignocellulosic composite door skin comprising a thickness from about 0.063 inches (1.60 mm) to 0.115 inches (2.92 mm).

5. The method of claim 4 , comprising pressing the mat to a thickness ranging from about 0.063 inches (1.60 mm) to about 0.114 inches (2.90 mm).

6. The method of claim 4 , comprising pressing the mat to a thickness ranging from about 0.090 inches (2.29 mm) to 0.114 inches (2.90 mm).

7. The method of claim 4 , comprising pressing the mat to a thickness ranging from about 0.100 inches (2.54 mm) to 0.110 inches (2.79 mm).

8. The method of claim 4 , further comprising adding a pre-press sealer to the at least one surface of the mat.

9. The method of claim 4 , wherein the lignocellulosic fiber comprises wood.

10. The method of claim 9 , wherein the wood used to generate the refined fibers comprises less than 22% fines, wherein fines comprise wood able to pass through a 1/16 inch by 1/16 inch (1.59 mm by 1.59 mm) mesh.

11. The method of claim 10 , wherein the door skin has a size of about 80 inches (1.52 m) in length and 36 inches (0.23 m) in width and a weight of less than or equal to 11 pounds (5.0 kg).

12. The method of claim 11 , wherein the resin comprises a formaldehyde-based resin or an isocyanate-based resin.

13. The method of claim 4 , wherein the thin-layer composite comprises a modulus of elasticity of ranging from about 250,000 psi to about 500,000 psi.

14. The method of claim 13 , wherein the reduction in lignocellulosic fiber per door skin results in a reduction in energy used to dry the fiber in the range of about 5% to 20% as compared to a door skin having a thickness of about 0.125 inches (3.175 mm).

15. The method of claim 4 , wherein the release agent is sprayed onto at least one surface of the mat.

16. The method of claim 4 , comprising a reduction in refined lignocellulosic fiber of up to 25% per door skin.

17. The method of claim 16 , wherein the reduction in lignocellulosic fiber per door skin results in a reduction in the workload for the refiner used to refine the fiber in the range of 5% to 20% as compared to a door skin having a thickness of about 0.125 inches (3.175 mm).

18. The method of claim 16 , wherein the reduction in lignocellulosic fiber per door skin results in a reduction in the amount of resin per door skin in the range of about 5% to 20% as compared to a door skin having a thickness of about 0.125 inches (3.175 mm).

19. The method of claim 16 , wherein the reduction in lignocellulosic fiber per door skin results in a reduction in the weight per door skin in the range of about 5% to 20% as compared to a door skin having a thickness of about 0.125 inches (3.175 mm).

20. The method of claim 4 , wherein the resin comprises a formaldehyde-based resin or an isocyanate-based resin.

21. The method of claim 4 , wherein the mixture comprises a release agent that is an aqueous emulsion of surfactants and polymers distinct from the wax.

22. The method of claim 21 , wherein the release agent is an internal release agent.

23. A method for making a molded thin-layer composite of reduced thickness comprising the steps of:

forming a mixture comprising a refined lignocellulosic fiber, a resin, and a wax selected from the group consisting of paraffin wax, microcrystalline wax, shellac wax, ozokerite wax, montan wax, slack wax, emulsified waxes thereof, and combinations thereof;

pre-pressing the mixture into a loose mat;

coating at least one of two dies with an anti-bonding agent including fluorocarbons; and

pressing the mat between the two dies at an elevated temperature and pressure and for sufficient time to form a thin-layer lignocellulosic composite comprising a thickness from about 0.063 inches (1.60 mm) to 0.115 inches (2.92 mm).

24. The method of claim 23 , wherein the resin comprises a formaldehyde-based resin or an isocyanate-based resin.

25. The method of claim 23 , wherein the mixture comprises an internal release agent that is an aqueous emulsion of surfactants and polymers distinct from the wax.

26. A method for making a door skin of reduced thickness comprising the steps of:

forming a mixture comprising a refined lignocellulosic fiber, a resin, and a wax selected from the group consisting of paraffin wax, microcrystalline wax, shellac wax, ozokerite wax, montan wax, slack wax, emulsified waxes thereof, and combinations thereof;

pre-pressing the mixture into a loose mat;

coating at least one of two dies with an anti-bonding agent including fluorocarbons; and

pressing the mat between the two dies at an elevated temperature and pressure and for sufficient time to form a thin-layer lignocellulosic composite door skin comprising a thickness from about 0.063 inches (1.60 mm) to 0.115 inches (2.92 mm).

27. The method of claim 26 , wherein the resin comprises a formaldehyde-based resin or an isocyanate-based resin.

28. The method of claim 26 , wherein the mixture comprises an internal release agent that is an aqueous emulsion of surfactants and polymers distinct from the wax.

Assignments (11)
RELEASE OF SECURITY INTEREST Recorded Aug 8, 2023
From: WILMINGTON TRUST
To: JELD-WEN, INC.
Reel/Frame 064523/0865 →
PATENT SECURITY AGREEMENT Recorded May 5, 2020
From: JELD-WEN, INC.
To: WILMINGTON TRUST, NATIONAL ASSOCIATION
Reel/Frame 052569/0935 →
SECURITY INTEREST Recorded Oct 24, 2014
From: JELD-WEN, INC.
To: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS ADMINISTRATIVE AGENT
Reel/Frame 034049/0001 →
SECURITY AGREEMENT Recorded Oct 20, 2014
From: JELD-WEN, INC.
To: BANK OF AMERICA, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 034017/0321 →
RELEASE OF SECURITY INTEREST Recorded Oct 17, 2014
From: BANK OF AMERICA, N.A.
To: JELD-WEN, INC.
Reel/Frame 034012/0942 →
RELEASE OF SECURITY INTEREST Recorded Oct 17, 2014
From: BANK OF AMERICA, N.A.
To: JELD-WEN, INC.
Reel/Frame 034012/0932 →
RELEASE OF SECURITY INTEREST Recorded Oct 17, 2014
From: BANK OF AMERICA, N.A.
To: JELD-WEN, INC.
Reel/Frame 034012/0921 →
NOTICE OF GRANT OF SECURITY INTEREST IN PATENTS Recorded Oct 5, 2011
From: JELD-WEN, INC.
To: BANK OF AMERICA, N.A., AS COLLATERAL AGENT
Reel/Frame 027017/0815 →
NOTICE OF GRANT OF SECURITY INTEREST IN PATENTS (SECOND LIEN) Recorded Oct 5, 2011
From: JELD-WEN, INC.
To: BANK OF AMERICA, N.A., AS COLLATERAL AGENT
Reel/Frame 027017/0833 →
NOTICE OF GRANT OF SECURITY INTEREST IN PATENTS Recorded Jul 16, 2009
From: JELD-WEN, INC.
To: BANK OF AMERICA, N.A., AS COLLATERAL AGENT
Reel/Frame 022960/0248 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 2, 2004
From: CLARK, RANDY JON; HENRY, MICHAEL JAY
To: JELD-WEN INC.
Reel/Frame 015759/0760 →