Method of reheat blow molding a container
View Patent ↗A method of reheat blow molding a container includes the step of positioning a preform in a blow mold cavity with at least one of the walls having an opening with an anvil received therein for movement between a first position outside the cavity and a second position at least partially within the cavity. Further, expanding the preform within the cavity while moving the anvil from its first position to its second position so that the expanding preform forms a pocket for receiving a handle therein.
1. A method of reheat blow molding a container, including the steps of: (a) positioning a preform in a blow mold cavity having a wall opening and an anvil disposed outside of said cavity and positioned to move into said cavity through said opening; (b) expanding said preform within said cavity by application of gas under pressure to said preform, and (c) during step (b), moving said anvil into said cavity through said opening at a time during said step (b) such that the expanding preform forms around said anvil; and initiating step (c) so that at least a portion of said preform is expanded laterally beyond said opening when said anvil initially contacts said preform.
2. The method of claim 1 including completing step (c) as said preform conforms to the shape defined by said mold cavity.
3. The method of claim 1 including timing said step (c) empirically with said step (b) so that said preform forms around said anvil without forming a hole in the expanding preform.
4. The method of claim 1 including moving said anvil into said mold cavity through said opening in a single motion.
5. The method of claim 4 including moving said anvil into said mold cavity through said opening at a substantially constant rate.
6. The method of claim 4 including moving said anvil into said mold cavity through said opening in a substantially linear path.
7. The method of claim 1 including initiating step (b) prior to initiating step (c).
8. The method of claim 7 wherein step (b) is initiated between 0.017 and 0.103 seconds before step (c) is initiated.
9. The method of claim 1 wherein said preform is of strain-hardenable plastic construction.
10. The method of claim 1 wherein said mold cavity is defined by at least two separable walls and said opening is located in a single one of said at least two separable walls.
11. The method of claim 10 including forming a pocket spaced from a parting line defined by said at least two separable walls.
12. A method of reheat blow molding a container, including the steps of:
(a) positioning a preform of strain-hardenable plastic construction in a blow mold cavity defined by at least two separable walls with at least one of said walls having an opening with an anvil received therein for movement between a first position outside said cavity and a second position at least partially within said cavity;
(b) expanding said preform within said cavity until said preform conforms substantially to the shape defined by said at least two walls, and
(c) during step (b), initiating movement of said anvil from said first position toward said second position after at least a portion of said preform is expanded laterally beyond said opening.
13. The method of claim 12 including timing step (c) empirically with step (b) so that said preform forms a continuous wall around said anvil without forming a hole in said preform.
14. The method of claim 12 including moving said anvil from said first position to said second position in a single motion.
15. The method of claim 12 including moving said anvil into its second position at generally the same time as said preform conforms substantially to the shape of said blow mold cavity.
16. The method of claim 12 wherein step (b) is initiated between 0.017 and 0.103 seconds before step (c) is initiated.
17. The method of claim 12 including arranging said opening in a single one of said at least two separable walls.
18. The method of claim 17 including forming a pocket spaced from a parting line defined by said at least two separable walls.