IP Library Granted Patent US 6,982,300
Granted Patent B2
US 6,982,300 · App. 10/893,827 · Granted Jan 3, 2006

Method for preparing a pressure sensitive adhesive formulation including an enhanced polyisobutylene modifier

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,982,300
App. No.
10/893,827
Granted
Jan 3, 2006
Kind
B2
Abstract

A method for preparing an improved pressure sensitive adhesive includes incorporating into a base polymer, an PIB modifier that is made up of a homopolymer of isobutylene wherein a predominant portion of the double bonds are in either an alpha position or a beta position. The modifier may function as a plasticizer, a tackifier extender or a combination plasticizer and tackifier extender for the pressure sensitive adhesive.

Claims (35)

1. A method for preparing a pressure sensitive adhesive having improved properties comprising providing a pressure sensitive adhesive base structure and including in said base structure a PIB modifier, said PIB modifier comprising a homopolymer of isobutylene wherein a predominant portion of the double bonds are in either an alpha position or a beta position.

2. A method as set forth in claim 1 , wherein said PIB modifier has a polydispersity no greater than about 2.2.

3. A method as set forth in claim 1 , wherein said PIB modifier has a M N no greater than about 3000.

4. A method as set forth in claim 3 , wherein said PIB modifier has a M N which is at least about 900.

5. A method as set forth in claim 1 , wherein at least about 92% of the monomeric units incorporated in the PIB modifier molecules are isobutylene moieties.

6. A method as set forth in claim 1 , wherein at least about 95% of the monomeric units incorporated in the PIB modifier molecules are isobutylene moieties.

7. A method as set forth in claim 1 , wherein at least about 99% of the monomeric units incorporated in the PIB modifier molecules are isobutylene moieties.

8. A method as set forth in claim 1 , wherein no more than about 1% of the monomeric units incorporated in the PIB modifier molecules are something other than isobutylene moieties.

9. A method as set forth in claim 1 , wherein at least about 40% of the double bonds of the PIB modifier molecules are in the alpha position.

10. A method as set forth in claim 1 , wherein at least about 50% of the double bonds of the PIB modifier molecules are in the alpha position.

11. A method as set forth in claim 1 , wherein at least about 60% of the double bonds of the PIB modifier molecules are in the alpha position.

12. A method as set forth in claim 1 , wherein at least about 70% of the double bonds of the PIB modifier molecules are in the alpha position.

13. A method as set forth in claim 1 , wherein at least about 80% of the double bonds of the PIB modifier molecules are in the alpha position.

14. A method as set forth in claim 1 , wherein at least about 90% of the double bonds of the PIB modifier molecules are in the alpha position.

15. A method as set forth in claim 1 , wherein more than 90% of the double bonds of the PIB modifier molecules are in the alpha position.

16. A method as set forth in claim 1 wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

17. A method as set forth in claim 9 wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

18. A method as set forth in claim 10 , wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

19. A method as set forth in claim 11 , wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

20. A method as set forth in claim 12 , wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

21. A method as set forth in claim 13 , wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

22. A method as set forth in claim 14 , wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

23. A method as set forth in claim 15 , wherein no more than about 1% of the double bonds of the PIB modifier molecules are in a position other than the alpha or beta.

24. A method as set forth in claim 1 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

25. A method as set forth in claim 2 wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

26. A method as set forth in claim 3 wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

27. A method as set forth in claim 6 wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

28. A method as set forth in claim 7 wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

29. A method as set forth in claim 10 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

30. A method as set forth in claim 11 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

31. A method as set forth in claim 12 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

32. A method as set forth in claim 13 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

33. A method as set forth in claim 14 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

34. A method as set forth in claim 15 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

35. A method as set forth in claim 16 , wherein from about 10 to about 60% by weight of said PIB modifier is included in said pressure sensitive adhesive.

Assignments (16)
RELEASE OF SECURITY INTEREST AT REEL/FRAME 29644/0870 Recorded Jun 8, 2022
From: BANK OF AMERICA, N.A., AS ADMINISTRATIVE AGENT
To: TPC GROUP LLC
Reel/Frame 060307/0955 →
TERMINATION AND RELEASE OF SECURITY INTEREST IN UNITED STATES TRADEMARKS AND PATENTS Recorded Aug 6, 2019
From: U.S. BANK NATIONAL ASSOCIATION, AS SUCCESSOR COLLATERAL AGENT TO WELLS FARGO BANK, NATIONAL ASSOCIATION
To: TPC GROUP LLC
Reel/Frame 049970/0375 →
CONFIRMATION OF SUCCESSION OF AGENCY Recorded Aug 5, 2019
From: WELLS FARGO BANK, NATIONAL ASSOCIATION
To: U.S. BANK NATIONAL ASSOCIATION
Reel/Frame 049962/0956 →
CONFIRMATION OF TERMINATION AND RELEASE OF SECURITY INTEREST IN PATENT RIGHTS Recorded Aug 2, 2019
From: DEUTSCHE BANK TRUST COMPANY AMERICAS
To: TPC GROUP LLC
Reel/Frame 049949/0182 →
RELEASE OF SECURITY INTEREST Recorded Jan 16, 2013
From: DEUTSCHE BANK TRUST COMPANY AMERICAS, AS COLLATERAL AGENT
To: TPC GROUP LLC
Reel/Frame 029639/0200 →
SECURITY AGREEMENT Recorded Jan 16, 2013
From: TPC GROUP LLC
To: BANK OF AMERICA, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 029644/0870 →
SECURITY AGREEMENT Recorded Jan 16, 2013
From: TPC GROUP LLC
To: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS COLLATERAL AGENT
Reel/Frame 029644/0910 →
SECURITY AGREEMENT Recorded Oct 14, 2010
From: TPC GROUP LLC (F/K/A TEXAS PETROCHEMICALS LP)
To: DEUTSCHE BANK TRUST COMPANY AMERICAS
Reel/Frame 025137/0398 →
RELEASE OF SECURITY INTEREST Recorded Oct 13, 2010
From: DEUTSCHE BANK TRUST COMPANY AMERICAS, AS COLLATERAL AGENT
To: TPC GROUP LLC
Reel/Frame 025126/0712 →
CERTIFICATE OF CONVERSION Recorded May 25, 2010
From: TEXAS PETROCHEMICALS LP
To: TEXAS PETROCHEMICALS LLC
Reel/Frame 024434/0263 →
CHANGE OF NAME Recorded May 25, 2010
From: TEXAS PETROCHEMICALS LLC
To: TPC GROUP LLC
Reel/Frame 024434/0363 →
RELEASE OF SECURITY INTEREST IN U.S. PATENTS Recorded May 5, 2010
From: U.S. BANK NATIONAL ASSOCIATION
To: TEXAS PETROCHEMICALS LP
Reel/Frame 024337/0518 →
GRANT OF SECURITY INTEREST IN U.S. PATENTS (REVOLVING LOAN) Recorded May 4, 2010
From: TPC GROUP LLC
To: DEUTSCHE BANK TRUST COMPANY AMERICAS, AS COLLATERAL AGENT
Reel/Frame 024329/0223 →
GRANT OF SECURITY INTEREST IN U.S. PATENTS (TERM LOAN) Recorded May 4, 2010
From: TPC GROUP LLC
To: DEUTSCHE BANK TRUST COMPANY AMERICAS, AS COLLATERAL AGENT
Reel/Frame 024329/0236 →
CHANGE OF NAME Recorded Feb 1, 2010
From: TEXAS PETROCHEMICALS LLC
To: TPC GROUP LLC
Reel/Frame 023870/0598 →
CONVERSION OF TEXAS PETROCHEMICALS LP Recorded Dec 18, 2008
From: TEXAS PETROCHEMICALS LP
To: TEXAS PETROCHEMICALS LLC
Reel/Frame 021998/0966 →