Fuel cell shutdown with steam purging
View Patent ↗The present invention relates to a method and apparatus for steam purging a solid oxide fuel cell stack. Purging the SOFC stack with steam has a physical flushing effect, removing carbon monoxide containing reformate and free oxygen gas from the anode area thereby reducing the potential for nickel oxide or nickel carbonyl formation.
1. A method of shutting down a solid oxide fuel cell stack having a fuel delivery subsystem and an air delivery subsystem, and having an anode comprising nickel, said method comprising the step of cooling the stack, or allowing the stack to cool, from an operating temperature of 600° C. to 1000° C. to an operating temperature of less than about 350° C. but above about 230° C. prior to purging with steam.
2. The method of claim 1 wherein the solid oxide fuel cell stack is cooled with process air through the air delivery subsystem.
3. The method of claim 1 wherein the fuel delivery subsystem comprises a steam reformer, and the steam purge is initiated by injecting water into the fuel delivery system at a water injection site upstream from the steam reformer.
4. The method of claim 3 further comprising the step of allowing a sacrificial material placed between the reformer and the water injection site to oxidize.
5. The method of claim 4 wherein the sacrificial oxidizable material comprises a metallic powder that upon oxidation increases hydrogen partial pressure and reduces oxygen partial pressure.