IP Library Granted Patent US 7,588,863
Granted Patent B2
US 7,588,863 · App. 10/925,086 · Granted Sep 15, 2009

Hologram recording method and hologram recording material

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,588,863
App. No.
10/925,086
Granted
Sep 15, 2009
Kind
B2
Abstract

To provide a hologram recording method capable of satisfying high sensitivity and at the same time, satisfying high diffraction efficiency, good preservability, low shrinkage percentage, dry processing and multiplex recording properties, a hologram recording method comprises a first step of producing a latent image upon holographic exposure, and a second step of causing a polymerization reaction due to the latent image, to form a interference fringe providing a refractive index modulation, wherein the first and second steps are dry process; particularly, the first step is a step of producing a colored material to form the latent image and the second step is a step of causing the polymerization reaction upon irradiating the colored material with a light having a wavelength different from that of the holographic exposure, to form the interference fringe providing the refractive index modulation.

Claims (32)

1. A hologram recording method, which comprises:

a first step of producing a latent image by holographic exposure of a hologram recording material, wherein the hologram recording material comprising a dye precursor that is a combination comprising at least an acid-induced color forming dye precursor and an acid generator; and

a second step of causing a polymerization reaction due to the latent image, so as to form a first interference fringe providing a refractive index modulation, wherein the latent image is a second interference fringe, the first interference fringe having a diffraction efficiency which is at least 5 times larger than that of the second interference fringe;

wherein each of the first step and the second step is dry process;

wherein the first step is a step of producing a colored material to form the latent image, the colored material having no absorption of a hologram reproducing light; and

the second step is a step of causing the polymerization reaction upon irradiating the colored material with a light which has a wavelength different from that of the holographic exposure, so as to form the first interference fringe providing the refractive index modulation,

wherein the light irradiated in the second step has a wavelength where a sensitizing dye, capable of being excited upon the holographic exposure in the first step, has a molar absorption coefficient of 5,000 or less.

2. The hologram recording method as claimed in claim 1 , wherein in the second step, the light irradiation is a non-imagewise exposure.

3. The hologram recording method as claimed in claim 1 , wherein the second step is a step of causing the polymerization reaction while the colored material is self sensitized or self amplified upon irradiating the colored material with a light which has a wavelength different from that of the holographic exposure, so as to form the first interference fringe providing the refractive index modulation.

4. The hologram recording method as claimed in claim 1 , which comprises fixing a sensitizing dye, capable of being excited upon the holographic exposure in the first step, by decomposing the sensitizing dye in the first step, the second step or a subsequent fixing step of at least one of light irradiation and heat application.

5. The hologram recording method as claimed in claim 1 , which comprises fixing a colored material to form the latent image, the colored material having no absorption of a hologram reproducing light, by decomposing the colored material in the second step or a subsequent fixing step of at least one of light irradiation and heat application.

6. A hologram recording method as claimed in claim 1 , which is a method for recording a volume phase hologram.

7. A hologram recording method as claimed in claim 1 , wherein in the first step, a multiplex hologram recording is performed by effecting the holographic exposure 10 times or more so as to the latent image.

8. A hologram recording method as claimed in claim 7 , wherein the multiplex hologram recording is performed under the common exposure amount.

9. A hologram recording material used in a hologram recording method according to claim 1 , the hologram recording material comprising:

a sensitizing dye capable of absorbing a light upon holographic exposure in the first step to be transformed into a first excited state;

a dye precursor capable of forming a colored material as a result of one of electron transfer and energy transfer from the first excited state of the sensitizing dye; or from a second excited state of the colored material, the second excited state of the colored material being formed in the second step, wherein the dye precursor is a combination comprising at least an acid-induced color forming dye precursor, an acid generator and an acid-increasing agent;

wherein the colored material has an absorption at a longer wavelength than a wavelength where the dye precursor has an absorption; and the colored material has no absorption of a hologram reproducing light;

a polymerizable compound;

a polymerization initiator capable of initiating polymerization of the polymerizable compound as a result of one of electron transfer and energy transfer from the first excited state of the sensitizing dye or from the second excited state of the colored material; and

a binder; and

an electron-donating compound having an ability of reducing a radial cation of the sensitizing dye, wherein the electron-donating compound is a phenothiazine compound.

10. The hologram recording material as claimed in claim 9 ,

wherein the polymerizable compound and the binder differ in refractive index; and

the polymerizable compound is capable of being photopolymerized to record a interference fringe in the hologram recording material, wherein when the polymerizable compound is photopolymerized to provide a polymerized compound, a composition ratio of the polymerizable compound or the polymerized compound to the binder is different between a bright portion of the interference fringe and a dark portion of the interference fringe, so as to form a interference fringe providing a refractive index modulation.

11. The hologram recording material as claimed in claim 9 , which is for an optical recording medium.

12. The optical recording medium, which comprises: a hologram recording material as claimed in claim 9 ; and a light-shielding cartridge, wherein the optical recording material is stored in a light-shielding cartridge during storage.

13. The hologram recording material as claimed in claim 9 , which is for a three-dimensional display.

14. The hologram recording material as claimed in claim 9 , which is for a holographic optical device.

15. The hologram recording material as claimed in claim 9 , wherein the acid-increasing agent is a compound represented by the following formula (4-1), (4-2), (4-3), (4-4), (4-5) or (4-6):

wherein R 101 represents a group of forming an acid having a pKa of 5 or less in the form of R 101 OH; R 102 represents a 2-alkyl-2-propyl group, a 2-aryl-2-propyl group, a cyclohexyl group, a tetrahydropyranyl group or a bis(p-alkoxyphenyl)methyl group; R 103 , R 104 , R 115 and R 117 each independently represents a substituent; R 105 , R 106 , R 107 , R 110 , R 113 and R 116 each independently represents a hydrogen atom or a substituent; R 118 and R 119 each independently represents an alkyl group and may combine with each other to form a ring; R 111 and R 112 represent alkyl groups which combine with each other to form a ring; R 114 represents a hydrogen atom or a nitro group; and n101 represents an integer of 0 to 3.

16. The hologram recording material as claimed in claim 15 , wherein in formulae (4-1) to (4-6), R 101 is a group of being a sulfonic acid or an electron-withdrawing group-substituted carboxylic acid in the form of R 101 OH.

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Nov 23, 2010
From: BANK OF AMERICA, N.A., AS SUCCESSOR-IN-INTEREST TO LASALLE BANK NATIONAL ASSOCIATION
To: CONTINENTAL STUCTURAL PLASTICS, INC.
Reel/Frame 025397/0374 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 15, 2007
From: FUJIFILM HOLDINGS CORPORATION (FORMERLY FUJI PHOTO FILM CO., LTD.)
To: FUJIFILM CORPORATION
Reel/Frame 018904/0001 →
SECURITY INTEREST Recorded Sep 14, 2006
From: CONTINENTAL STRUCTURAL PLASTICS, INC.
To: LASALLE BANK, NATIONAL ASSOCIATION, AS AGENT
Reel/Frame 018260/0786 →