IP Library Granted Patent US 7,628,040
Granted Patent B2
US 7,628,040 · App. 10/947,679 · Granted Dec 8, 2009

Method for joining an optical fiber and an optical lens

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,628,040
App. No.
10/947,679
Granted
Dec 8, 2009
Kind
B2
Abstract

In the jointing method of jointing an optical fiber F a softening point of which is higher than an optical lens L to the optical lens L, only the optical lens is softened by heating, and an end face as a joint portion of the optical fiber is pushed into a joint portion of the softened optical lens to thereby joint them.

Claims (16)

1. A method for jointing an optical fiber with an optical lens, comprising the steps of:

heating an end portion of a core wire of the optical fiber up to a softening point of the optical fiber so that a rounded surface is formed at the end portion of the core wire;

heating a jointed portion of the optical lens so as not to exceed a softening point of the optical lens;

pushing the core wire of the optical fiber, in which the rounded surface is formed at the end portion, into the softened jointed portion of the optical lens; and

cooling the jointed portion of the optical lens so that the core wire of the optical fiber is fastened by the jointed portion of the optical lens and they are joined together;

wherein the softening point of the optical fiber is higher than the softening point of the optical lens.

2. The method of claim 1 , further comprising, prior to pushing the core wire of the optical fiber into the softened jointed portion of the optical lens,

arranging the end portion of the optical fiber and the joint portion of the optical lens to be opposed to each other; and

softening the optical lens by a heat source that is located apart from the joint portion of the optical lens and the optical fiber.

3. The method of claim 2 , wherein the heat source is an arc discharge.

4. The method of claim 2 , wherein the heat source is located apart from the optical fiber and the optical lens in a radial direction of a longitudinal axis of the optical fiber.

5. The method of claim 1 , further comprising:

applying a tensile force on the jointed optical fiber and the optical lens in a direction to stretch the optical fiber and the optical lens; and

inspecting a jointed condition between the optical lens and the optical fiber based on the tensile force applied thereto.

6. The method of claim 1 , further comprising heating the end portion of the core wire of the optical fiber until it is determined that the end portion becomes the rounded surface.

7. The method of claim 1 , further comprising moving the optical lens to a position where the end portion of the core wire is in contact with the optical lens after heating the end portion of the core wire of the optical fiber.

Assignments (1)
CHANGE OF NAME Recorded Jan 25, 2017
From: CITIZEN HOLDINGS CO., LTD.
To: CITIZEN WATCH CO., LTD.