Emissions treatment system with NSR and SCR catalysts
Provided is an emissions treatment system for an exhaust stream, having a NOx storage reduction (NSR) catalyst with a NOx sorbent at a concentration of at least 0.1 g/in 3 and a platinum group metal component dispersed on a refractory metal oxide support; and, an SCR catalyst disposed downstream of the NSR catalyst. The emissions treatment system is advantageously used for the treatment of exhaust streams from diesel engines and lean burn gasoline engines.
1. A method for converting NOx in an exhaust gas from a diesel engine or lean burn gasoline engine to N 2 , comprising:
(a) contacting the exhaust gas comprising NOx in a lean period with a NOx storage reduction (NSR) catalyst comprising a platinum group metal component and at least 0.1 g/in 3 of a NOx sorbent, selected from the group consisting essentially of alkali and alkaline earth metal oxides dispersed on a refractory metal oxide to sorb a portion of NOx in the form of alkaline earth metal nitrate from the exhaust gas and allowing a portion of the NOx to flow through the NSR catalyst untreated;
(b) periodically altering the air/fuel ratio of the exhaust stream to provide a rich gaseous stream during a rich period;
(c) contacting the rich gaseous stream with the NSR catalyst to reduce the sorbed NOx to NH 3 ; and,
(d) subsequently contacting a mixture of the NH 3 and the untreated NOx in the exhaust gas with an SCR catalyst to form N 2 , wherein the NSR further comprises an oxygen storage component selected from one or more oxides of cerium and praseodymium in an amount less than 0.5 g/in 3 .
2. The method of claim 1 , wherein the SCR catalyst is located on a filter.
3. The method of claim 2 , wherein the NSR catalyst is located on the same filter upstream of the SCR catalyst.
4. The method of claim 1 , wherein the NSR catalyst comprises at least 0.05 g/in 3 of an oxygen storage component.
5. The method of claim 1 , further comprising step (c 1 ), following step (c), wherein step (c 1 ) comprises sorbing a portion of the NH 3 on the SCR catalyst.
6. The method of claim 1 , wherein the alteration of the air/fuel ratio of the exhaust gas stream in (b), comprises injecting a reducing agent selected from at least one of a hydrocarbon fuel, carbon monoxide and hydrogen into the exhaust gas upstream of the NSR catalyst.
7. The method of claim 1 , wherein the exhaust gas of (a) has a space velocity of 10,000 to 200,000 h −1 through the NSR catalyst.
8. The method of claim 1 , wherein the exhaust gas of (d) has a space velocity of 10,000 to 200,000 h −1 through the SCR catalyst.
9. The method of claim 1 , wherein the λ of the rich gaseous stream is from 0.80 to 0.995.
10. The method of claim 1 , wherein the λ of the exhaust gas during lean period is greater than 1.1.
11. The method of claim 1 , wherein the rich period is from 1 to 50% of the lean period.
12. The method of claim 1 , wherein the exhaust gas of (a) has a temperature of 100 to 6000° C.