IP Library Granted Patent US 7,562,539
Granted Patent B2
US 7,562,539 · App. 11/011,130 · Granted Jul 21, 2009

Method and the device for making high precision coating of insert for glass molding

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,562,539
App. No.
11/011,130
Granted
Jul 21, 2009
Kind
B2
Abstract

A method for making high precision hard film coating on a mold core comprises the following steps of: (a) providing a mold jig ( 200, 300 ) and a mold core ( 208, 308 ); (b) defining a through hole ( 206, 364 ) of a first inner diameter in the mold jig; (c) forming a rim ( 254, 354 ) of a second inner diameter on the inner side of the through hole, the second inner diameter being smaller than the first inner diameter; (d) configuring the mold core into a mold core including a body ( 212, 312 ) of a first external diameter and a top portion ( 250, 350 ) of a second external diameter, the second external diameter being smaller than the first external diameter to define a shoulder ( 252, 352 ) between the body and the top portion, the first external diameter being substantially equal to the first inner diameter and larger than the second inner diameter, the second external diameter being substantially equal to or smaller than the second inner diameter; and (e) coreing the mold core into the through hole of the mold jig from the bottom, the shoulder of the mold core engaging with the rim, the upper surface of the top portion of the mold core being substantially flush with the upper surface of the mold jig, and a groove ( 256, 356 ) being defined between the inner side of the through hole and the outer side of the top portion of the mold core. A device for performing this method is also disclosed.

Claims (12)

1. A method for making high precision film coating on a mold core comprising the following steps:

(1) providing a mold jig and a mold core to be received in the mold jig;

(2) defining a through hole of a first inner diameter in the mold jig for receiving the mold core therein;

(3) forming a rim of a second inner diameter on the inner side of the through hole of the mold jig, the second inner diameter being smaller than the first inner diameter of the through hole;

(4) forming a body of a first external diameter and a top portion of a second external diameter in the mold core, the second external diameter being smaller than the first external diameter to define a shoulder between the body and the top portion, the first external diameter being substantially equal to the first inner diameter of the through hole of the mold jig and larger than the second inner diameter of the rim of the mold jig, the second external diameter being substantially equal to or smaller than the second inner diameter of the rim;

(5) inserting the mold core into the through hole of the mold jig from a bottom of the mold jig, wherein firstly the top portion, the shoulder and the body of the mold core are successively inserted into the through hole of the first inner diameter from the bottom of the mold jig, and then the top portion of the second external diameter passes through the rim of the second inner diameter, and finally the shoulder of the mold core engages with the rim of the mold jig, the body of the first external diameter being received in the through hole of the first inner diameter, the upper surface of the top portion of the second external diameter being substantially flush with the upper surface of the mold jig, and a groove being defined between the inner side of the through hole of the first inner diameter and the outer side of the top portion of the second external diameter; and

(6) coating the mold core to form a side hard film on the outer side surface of the top portion of the second external diameter and a hard film on the upper surface of the top portion of the second external diameter.

2. The method for making high precision film coating on a mold core as claimed in claim 1 , wherein the distance between the shoulder of the mold core and the upper surface of the top portion of the mold core is approximately in the range of 1 mm to 2 mm.

3. The method for making high precision film coating on a mold core as claimed in claim 1 , wherein the through hole of the mold jig is configured by a bushing in the mold jig.

4. The method for making high precision film coating on a mold core as claimed in claim 3 , wherein the bushing comprises an outwardly projecting flange at the bottom thereof, the flange abutting against a lower surface of the mold jig.

5. The method for making high precision film coating on a mold core as claimed in claim 3 , wherein the mold core comprises a base connected with the body, the base having an outwardly projecting flange abutting against a lower surface of the bushing.

6. The method for making high precision film coating on a mold core as claimed in claim 3 , wherein the bushing has an upper surface substantially flush with the upper surface of the mold core.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 24, 2012
From: ASIA OPTICAL CO., INC.
To: ASIA OPTICAL INTERNATIONAL LTD.
Reel/Frame 028842/0757 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 15, 2004
From: WANG, KUN-CHIH
To: ASIA OPTICAL CO., INC.
Reel/Frame 016092/0930 →