IP Library Granted Patent US 7,400,803
Granted Patent B2
US 7,400,803 · App. 11/090,656 · Granted Jul 15, 2008

Method and apparatus for providing a hydrogen diffusion barrier for fiber optic cables used in hostile environments

Assignee: Welldynamics, B.V.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,400,803
App. No.
11/090,656
Granted
Jul 15, 2008
Kind
B2
Abstract

A fiber optic conduit for use in a hostile environment includes an axial tube. The axial tube comprises a corrosion resistant material and is operable to receive one or more optical fibers. The fiber optic conduit further includes a hydrogen barrier shell that is disposed in contact with the axial tube. The hydrogen barrier shell comprises a material that is capable of reducing hydrogen permeation through the fiber optic conduit and has a thickness of at least approximately one-thousandth of an inch.

Claims (28)

1. A fiber optic conduit for use in a hostile environment, comprising:

an axial tube comprising a corrosion resistant material and operable to receive one or more optical fibers; and

a hydrogen barrier shell disposed in contact with the axial tube, the hydrogen barrier shell comprising a material capable of reducing hydrogen permeation through the fiber optic conduit and a thickness of at least approximately one-thousandth of an inch.

2. The fiber optic conduit of claim 1 , wherein the axial tube operates as a hydrostatic pressure boundary for fiber optic conduit.

3. The fiber optic conduit of claim 1 , wherein the hydrogen barrier shell adheres to the axial tube through an interference fit.

4. The fiber optic conduit of claim 1 , wherein the hydrogen barrier shell is capable of reducing ionizing radiation flux intensity through the fiber optic conduit.

5. The fiber optic conduit of claim 1 , wherein the material capable of reducing hydrogen permeation through the fiber optic conduit is selected from the group consisting of carbon, silicon, germanium, tin, lead, and gold.

6. The fiber optic conduit of claim 1 , wherein the hydrogen barrier shell forms a cylindrical covering substantially about the axial tube.

7. The fiber optic conduit of claim 6 , wherein the hydrogen barrier shell forms a cylindrical covering substantially about an inner surface of the axial tube.

8. The fiber optic conduit of claim 6 , wherein the hydrogen barrier shell forms a cylindrical covering substantially about an outer surface of the axial tube.

9. The fiber optic conduit of claim 1 , wherein the hydrogen barrier shell is substantially free from relying on the axial tube for mechanical integrity.

10. A method of forming a fiber optic conduit capable of being used in a hostile environment, the method comprising:

forming an axial tube a corrosion resistant material and operable to receive one or more optical fibers;

forming a barrier layer comprising a material capable of reducing hydrogen permeation through the fiber optic conduit; and

after forming the barrier layer, forming a hydrogen barrier shell disposed in contact with the axial tube, wherein forming a hydrogen barrier shell comprises forming an interference fit between the barrier layer and the axial tube.

11. The method of claim 10 , wherein forming an interference fit between the barrier layer and the axial tube comprises expanding the barrier layer using a mini-expandable pig.

12. The method of claim 10 , wherein forming an interference fit between the barrier layer and the axial tube comprises passing the combination of the axial tube and the barrier layer through a swage die.

13. The method of claim 10 , wherein the hydrogen barrier shell is substantially free from relying on the inner axial tube for mechanical integrity.

14. The method of claim 10 , wherein the hydrogen barrier shell comprises a thickness at least approximately one-thousandth of an inch.

15. A fiber optic conduit for use in a hostile environment, comprising:

an axial tube comprising a corrosion resistant material and capable of receiving one or more optical fibers; and

a hydrogen barrier shell comprising a material capable of reducing hydrogen permeation through the fiber optic conduit and operable to form a cylindrical covering substantially about a surface of the axial tube,

wherein at least a portion of the hydrogen barrier shell is in contact with and adheres to at least a portion of the axial tube through an interference fit, and

wherein the hydrogen barrier shell is substantially free from relying on the axial tube for mechanical integrity.

16. The fiber optic conduit of claim 15 , wherein the hydrogen barrier shell forms a cylindrical covering substantially about an inner surface of the axial tube.

17. The fiber optic conduit of claim 15 , wherein the hydrogen barrier shell forms a cylindrical covering substantially about an outer surface of the axial tube.

18. The fiber optic conduit of claim 15 , wherein the hydrogen barrier shell is capable of reducing radiation permeation through the fiber optic conduit.

19. The fiber optic conduit of claim 15 , wherein the thickness of the hydrogen barrier shell comprises at least approximately one-thousandth of an inch.

Assignments (4)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 5, 2007
From: HALLIBURTON ENERGY SERVICES, INC.
To: WELLDYNAMICS, B.V.
Reel/Frame 019781/0406 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 24, 2007
From: MAIDA, JOHN L., JR., MR.
To: HALLIBURTON ENERGY SERVICES, INC.
Reel/Frame 018800/0504 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 18, 2007
From: HALLIBURTON ENERGY SERVICES, INC.
To: WELLDYNAMICS, B.V.
Reel/Frame 018767/0859 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 8, 2005
From: MADIA, JOHN L. JR.
To: HALLIBURTON ENERGY SERVICES, INC.
Reel/Frame 016770/0773 →
Continuity (1)
Related Publication 20060215974A1 · Sep 28, 2006