IP Library Granted Patent US 7,421,775
Granted Patent B2
US 7,421,775 · App. 11/173,618 · Granted Sep 9, 2008

Method of manufacturing antenna for RFID tag

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,421,775
App. No.
11/173,618
Granted
Sep 9, 2008
Kind
B2
Abstract

A method of easily and inexpensively manufacturing an antenna for an RFID tag by forming the antenna using magnets of a pattern corresponding to a shape of the antenna is provided. One example method includes a) placing a substrate above a level of a fluid containing a conductive substance, b) placing a magnet (e.g., an electromagnet including an electrode) formed in a shape of an antenna pattern above a surface of the substrate, and adhering the conductive substance to a bottom of the substrate in the shape of the antenna pattern by a magnetic force, and c) fixing the conductive substance adhered to the bottom of the substrate.

Claims (11)

1. A method of manufacturing an antenna for an RFID tag, the method comprising:

orienting at least one magnet configured to produce a magnetic field that has a desired antenna shape above and substantially proximate to a container holding a fluid containing a conductive substance to attract the conductive substance from the container;

disposing a nonconductive substrate between the at least one magnet and the container;

forming a conductive pattern corresponding to the antenna shape of the magnetic field on a bottom surface of the nonconductive substrate; and

fixing the formed conductive pattern to the bottom surface of the nonconductive substrate to form the antenna.

2. The method of claim 1 wherein the orienting step comprises arranging a plurality of magnets in an array so that a plurality of conductive patterns are formed simultaneously on the bottom surface of the nonconductive substrate.

3. The method of claim 2 further comprising, after the fixing step, the step of separating the plurality of conductive patterns from each other.

4. The method of claim 1 wherein the forming step comprises energizing the at least one magnet to produce the magnetic field.

5. The method of claim 4 wherein the energizing step persists during the fixing step.

6. The method of claim 1 wherein the fixing step comprises applying a fixing liquid on the conductive pattern.

7. The method of claim 1 wherein the fixing step comprises attaching a protective sheet on the conductive pattern.

Assignments (3)
CORRECTIVE ASSIGNMENT TO CORRECT THE RECEIVING PARTY ADDRESS PREVIOUSLY RECORDED AT REEL: 036714 FRAME: 0757. ASSIGNOR(S) HEREBY CONFIRMS THE CHANGE OF NAME. Recorded Nov 9, 2015
From: SAMSUNG TECHWIN CO., LTD.
To: HANWHA TECHWIN CO., LTD.
Reel/Frame 037072/0008 →
CHANGE OF NAME Recorded Sep 29, 2015
From: SAMSUNG TECHWIN CO., LTD.
To: HANWHA TECHWIN CO., LTD.
Reel/Frame 036714/0757 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 8, 2005
From: KWAK, JAE-HYUN; LIM, SE-JIN; KIM, SOO-HO
To: SAMSUNG TECHWIN CO., LTD.
Reel/Frame 016617/0103 →