IP Library Granted Patent US 7,457,027
Granted Patent B2
US 7,457,027 · App. 11/185,261 · Granted Nov 25, 2008

Fabrication of cell cavities for electrooptic devices

Assignee: ElectroChromix, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,457,027
App. No.
11/185,261
Granted
Nov 25, 2008
Kind
B2
Abstract

This invention discloses methods to dispense adhesives for fabricating electrooptic devices. In addition the invention also discloses on how the cavities of these electrooptic devices may be filled using detachable tabs. The Electrooptic devices of this invention may comprise liquid or solid electrolytes.

Claims (16)

1. A method of producing a cell for an electrochromic device comprising front and rear spaced elements, each having front and rear surfaces and a seal member bonding said front and rear elements together in a spaced apart relationship to define a chamber with at least one vent and one inlet that is at least partially formed in a detachable tab, wherein the method comprises injecting an electrolyte composition in liquid state into the chamber via the inlet and then closing the inlet and the vent.

2. A method of producing a cell for an electrochromic device comprising front and rear spaced elements, each having front and rear surfaces and a seal member bonding said front and rear elements together in a spaced apart relationship to define a chamber, wherein the method comprises injecting a liquid electrolyte in the chamber via a detachable tab, wherein a sealant is applied to at least one of the front and rear surfaces in a manner that forms a vent and a fluid inlet at the detachable tab, and injecting liquid electrolyte into the chamber via the fluid inlet at the detachable tab.

3. A method as set forth in claim 2 , wherein the vent is at least partially formed in the sealant.

4. A method as set forth in claim 3 , including closing the vent when the chamber is filled with the liquid electrolyte.

5. A method as set forth in claim 3 , including detaching the tab to form a gap in the sealant, and then closing the gap in the sealant.

6. A method as set forth in claim 5 , wherein the injected electrolyte comprises an electrolyte that solidifies in the chamber by formation of multiphase structure.

7. A method as set forth in claim 5 , wherein the injected electrolyte comprises an electrolyte that solidifies in the chamber by formation of cross links.

8. An electrochromic mirror device comprising front and rear spaced elements, each having front and rear surfaces and a seal member bonding said front and rear elements together in a spaced apart relationship to define a chamber with at least one vent and one inlet, wherein the said chamber is filled by injecting an electrolyte composition in liquid state via an inlet in a detachable tab.

9. An electrochromic mirror device as in claim 8 wherein the electrolyte is solidified after the chamber is filled.

10. An electrochromic mirror device as in claim 9 where the solidification occurs via any one of multpiphase formation or polymerization.

11. An electrochromic mirror device as in claim 8 wherein the electrolyte is injected at an elevated temperature.

12. An electrochromic mirror device as in claim 8 , wherein the said chamber is preheated prior to the filling process.

13. An electrochromic mirror device as in claim 8 , wherein the electrolyte composition is injected at a pressure between 5 and 50 psi.

14. An electrochromic mirror device as in claim 8 , wherein the chamber is clamped during the injection process.

15. A method of producing a cell for an electrochromic mirror device comprising front and rear spaced elements, each having front and rear surfaces and a seal member bonding said front and rear elements together in a spaced apart relationship to define a chamber wherein the method comprises injecting an electrolyte in the liquid state into the chamber via an inlet in a detachable tab and wherein the said injection process further comprises of sealing the nozzle of the injection device against the said inlet during the said injection process.

16. A method of producing a cell for an electrochromic mirror device as in claim 15 wherein the chamber is flushed with an inert gas prior to the electrolyte injection process.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 28, 2011
From: ELECTROCHROMIX, INC.
To: AJJER, LLC
Reel/Frame 026034/0935 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 21, 2005
From: LECOMPTE, ROBERT S.; LOPEZ TONAZZI, JUAN CARLOS
To: ELECTROCHROMIX. INC.
Reel/Frame 016828/0168 →
Continuity (2)
Provisional Application 6058949200 · Jul 20, 2004
Related Publication 20060027260A1 · Feb 9, 2006