IP Library Granted Patent US 7,147,999
Granted Patent B2
US 7,147,999 · App. 11/209,733 · Granted Dec 12, 2006

Photothermographic material

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,147,999
App. No.
11/209,733
Granted
Dec 12, 2006
Kind
B2
Abstract

The present invention provides a photothermographic material, comprising a photosensitive silver halide, a non-photosensitive organic solvent salt, a reducing agent for a silver ion, and a binder on one face of a support, for being applied by using an organic solvent, the photothermographic material further comprising at least one compound selected from the group of compounds consisting of: a compound represented by the following general formula (1), a compound having a β-lactam ring, a compound having a group that is adsorptive to a silver halide and a group that reduces a silver halide and a precursor thereof:

Claims (19)

1. A photothermographic material comprising, on one surface of a support, a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent for a silver ion, and a binder, which are applied to the support using an organic solvent, wherein the photosensitive silver halide has a silver iodide content of 90% by mol to 100% by mol, and the photothermographic material further comprises a compound represented by formula (4):

E-(W)n-F  Formula (4)

wherein in formula (4),

E represents an atomic group containing a group that can be adsorbed to a silver halide and E is mercaptotriazole or mercaptotetrazole; W represents a divalent linking group; n represents 0 or 1; and F represents a reducing group derived from a hydroxyurea or a phenidone.

2. The photothermographic material according to claim 1 , wherein the reducing group represented by F in formula (4) is a group derived from a hydroxyurea.

3. The photothermographic material according to claim 1 , wherein an average grain size of the photosensitive silver halide is from 5 nm to 50 nm.

4. The photothermographic material according to claim 1 comprising, as the binder, polyvinyl butyral in an amount of 50% by weight to 100% by weight based on a total binder component in a photosensitive layer which is provided on the support.

5. A photothermographic material comprising, on one surface of a support, a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent for a silver ion, and a binder, which are applied to the support using an organic solvent, wherein a silver iodide content of the photosensitive silver halide is from 90% by mol to 100% by mol and the photothermographic material further comprises a compound represented by formula (1):

wherein in formula (1),

Y represents a hydroxyl group or an —NL 2 L 3 group, in which L 2 and L 3 may be same as or different from each other and each independently represent a hydrogen atom, an alkyl group, or an aryl group;

L 1 represents a sulfur-containing saturated heterocyclic residue, an alkyl group, an aryl group, a hydrogen group, or a group represented by A-S—B in which A represents an alkylene group and B represents a hydrogen atom, an alkyl group, or an aryl group; and

Z represents an atomic group required for forming a 5- or 6-membered carbon ring which may have a substituent.

6. The photothermographic material according to claim 5 , wherein a content of silver iodide in the photosensitive silver halide is from 40% by mol to 100% by mol.

7. The photothermo graphic material according to claim 5 , wherein an average grain diameter of the photosensitive silver halide is from 5 nm to 80 nm.

8. The photothermographic material according to claim 5 , wherein L 1 in formula (1) represents a sulfur-containing saturated heterocyclic residue or a group represented by A-S—B.

9. The photothermographic material according to claim 5 , wherein Z in formula (1) represents an atomic group required for forming a 6-membered carbon ring.

10. The photothermographic material according to claim 5 , wherein Y in formula (1) represents a hydroxyl group.

11. The photothermographic material according to claim 5 comprising, as the binder, polyvinyl butyral in an amount of 50% by weight to 100% by weight based on a total binder component in a photosensitive layer which is provided on the support.

12. The photothermographic material according to claim 1 , wherein the reducing group represented by F in formula (4) is a group derived from a phenidone.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 24, 2007
From: FUJIFILM HOLDINGS CORPORATION (FORMERLY FUJI PHOTO FILM CO. LTD.)
To: FUJIFILM CORPORATION
Reel/Frame 019331/0493 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 2, 2005
From: OHZEKI, TOMOYUKI; MIFUNE, HIROYUKI; INABA, TADASHI; YAMADA, KOHZABUROH; WATANABE, KATSUYUKI
To: FUJI PHOTO FILM CO., LTD.
Reel/Frame 018530/0151 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 2, 2005
From: OHZEKI, TOMOYUKI; MIFUNE, HIROYUKI; INABA, TADASHI; YAMADA, KOHZABUROH; WATANABE, KATSUYUKI
To: FUJI PHOTO FILM CO., LTD.
Reel/Frame 017224/0146 →