Full-color active matrix organic electroluminescent device, fabrication method thereof and electronic devices employing the same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,538,489
App. No.
11/271,555
Granted
May 26, 2009
Kind
B2
Abstract

A full-color active matrix organic electroluminescent device and fabrication method thereof. The full-color active matrix organic electroluminescent device includes a substrate with a plurality of TFTs, a buffer layer formed on the substrate beyond the TFTs, a color filter formed on the buffer layer, a flat layer formed on the entire surface of the color filter, a first electrode formed on the flat layer, an organic electroluminescent layer formed on the first electrode, and a second electrode formed on the organic electroluminescent layer, wherein the flat layer is formed by a low temperature thin film process.

Claims (23)

1. A color active matrix organic electroluminescent device, comprising a plurality of pixel areas arranged in a matrix, each pixel area comprising:

a thin film transistor formed on a substrate;

a buffer layer formed on the substrate beyond the thin film transistor;

a color filter formed on the buffer layer;

a flat layer formed on the color filter;

a first electrode formed on the flat layer and electrically connected to the thin film transistor;

an organic electroluminescent layer formed on the first electrode; and

a second electrode formed on the organic electroluminescent layer.

2. The device as claimed in claim 1 , wherein the flat layer is fanned by a low temperature thin film process.

3. The device as claimed in claim 2 , wherein the low temperature thin film process has an operating temperature not more than 350° C.

4. The device as claimed in claim 1 , wherein the surface roughness of the flat layer is less than 10 nm.

5. The device as claimed in claim 1 , wherein the flat layer has a thickness more than 10 times larger than the surface roughness of the color filter.

6. The device as claimed in claim 2 , wherein the low temperature thin film process is liquid phase deposition., spin-on coating, or sputtering.

7. The device as claimed in claim 2 , wherein the law temperature thin film process is low temperature magnetron sputtering.

8. The device as claimed in claim 1 , wherein the flat layer is low temperature dielectric layer or spin-on glass.

9. An electronic device, comprising

a color active matrix organic electroluminescent device as claimed in claim 2 ; and

a controller, wherein the controlleroperatively couples to the full-color active matrix organic electroluminescent device.

10. The device as claimed in claim 1 , wherein the first electrode is formed directly on the flat layer.

11. The device as claimed in claim 1 , wherein the first electrode is formed directly on and touching the flat layer.

12. The device as claimed in claim 1 , wherein the first electrode is formed on the flat layer with out an intervening layer.

13. The device as claimed in claim 1 , wherein the flat layer has a planarized surface on which the first electrode is formed.

14. The device as claimed in claim 1 , wherein the flat layer has a smooth top surface on which the first electrode is formed.