Solid-free-form fabrication process and apparatus including in-process workpiece cooling

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,326,377
App. No.
11/292,391
Granted
Feb 5, 2008
Kind
B2
Abstract

A solid free form fabrication system for manufacturing a component by successively building feedstock layers representing successive cross-sectional component slices includes a platform for receiving and supporting the feedstock layers, a feedstock supplying apparatus that deposits the feedstock into a predetermined region to form the feedstock layers, an energy source directed toward the predetermined region to modify the feedstock in the predetermined region and thereby manufacture the component, and a temperature control block disposed on the platform and directly in contact with the deposited feedstock layers to modify the feedstock temperature while manufacturing the component. A solid free form fabrication method uses the system to manufacture the component from the feedstock material

Claims (37)

1. A solid free form fabrication system for manufacturing a component by successively building feedstock layers representing successive cross-sectional component slices, the system comprising:

a platform for receiving and supporting the feedstock layers;

a feedstock supplying apparatus that deposits the feedstock into a predetermined region to form the feedstock layers;

an energy source directed toward the predetermined region to modify the feedstock in the predetermined region and thereby manufacture the component; and

a temperature control block disposed on the platform and directly in contact with the deposited feedstock layers to modify the feedstock temperature while manufacturing the component.

2. The solid free form fabrication system of claim 1 , wherein the system is an ion fusion formation system, the energy source is a plasma torch positioned to emit a plasma stream in a plasma path, and the feedstock supplying apparatus is operably configured to direct the feedstock into the plasma path and to the predetermined region to form the feedstock layers.

3. The solid free form fabrication system of claim 1 , wherein the temperature control block is formed from a metal selected from the group consisting of copper, aluminum, and silicon carbide.

4. The solid free form fabrication system of claim 1 , further comprising:

a fluid reservoir containing a fluid; and

a fluid circulation channel in fluid communication with the fluid reservoir, and adapted to change the temperature of the temperature control block using the fluid.

5. The solid free form fabrication system of claim 4 , wherein the fluid circulation channel includes at least one fluid passage formed inside the temperature control block.

6. The solid free form fabrication system of claim 4 , wherein the fluid circulation channel includes at least one fluid circulation coil that contacts the control block exterior.

7. The solid free form fabrication system of claim 4 , further comprising:

a temperature sensor that measures the control block temperature and transmits temperature data representative thereof; and

a processor that receives the temperature data and, responsive thereto, regulates fluid flow from the fluid reservoir to the fluid circulation channel.

8. The solid free form fabrication system of claim 4 , wherein the fluid is a liquid that is substantially cooler than the ambient temperature surrounding the temperature control block.

9. The solid free form fabrication system of claim 4 , wherein the fluid is a liquid that is substantially hotter than the ambient temperature surrounding the temperature control block.

10. The solid free form fabrication system of claim 1 , further comprising:

a fan that blows a column of a gas onto the deposited feedstock layers while manufacturing the component.

11. The solid free form fabrication system of claim 1 , wherein the temperature control block is heated by electrical resistance.

12. The solid free form fabrication system of claim 1 , further comprising an energy source that directs radiation onto the deposited feedstock layers while manufacturing the component.

13. A solid free form fabrication method for manufacturing a component from a feedstock material, the method comprising:

forming successive feedstock layers by depositing the feedstock material into a predetermined region on a platform, the feedstock layers representing successive cross-sectional component slices;

modifying the feedstock by directing an energy source to the predetermined region and thereby forming the component; and

controlling the temperature of the component being formed by contacting the feedstock layers with a temperature control block disposed on the platform.

14. The solid free form fabrication method of claim 13 , performed using an ion fusion formation system, wherein the energy source is a plasma torch positioned to emit a plasma stream in a plasma path, and the feedstock is directed into the plasma path and to the predetermined region to form the feedstock layers.

15. The solid free form fabrication method of claim 13 , further comprising:

adjusting the temperature of the temperature control block using a fluid circulation channel that receives a pressurized fluid from a fluid reservoir.

16. The solid free form fabrication method of claim 14 , wherein the fluid circulation channel includes at least one fluid passage formed inside the temperature control block.

17. The solid free form fabrication method of claim 14 , wherein the fluid circulation channel includes at least one fluid circulation coil that contacts the control block exterior.

18. The solid free form fabrication method of claim 15 , further comprising:

measuring the control block temperature; and

automatically regulating flow from the fluid reservoir to the fluid circulation channel in response to the measured control block temperature.

19. The solid free form fabrication method of claim 13 , further comprising:

blowing a column of a gas onto the deposited feedstock while manufacturing the component.

20. The solid free form fabrication method of claim 13 , further comprising:

directing radiation from an energy source onto the deposited feedstock layers while manufacturing the component.

Assignments (9)
RELEASE OF SECURITY INTEREST Recorded Jan 24, 2022
From: NTI HOLDINGS AS
To: NORSK TITANIUM AS
Reel/Frame 058741/0347 →
RELEASE OF SECURITY INTEREST Recorded Jan 24, 2022
From: NTI HOLDINGS AS
To: NORSK TITANIUM AS
Reel/Frame 058741/0742 →
RELEASE OF SECURITY INTEREST Recorded Jan 24, 2022
From: NTI HOLDING AS
To: NORSK TITANIUM AS
Reel/Frame 058742/0245 →
INTELLECTUAL PROPERTY SECURITY AGREEMENT (UNITED STATES) Recorded Feb 2, 2021
From: NORSK TITANIUM AS
To: NTI HOLDINGS AS, AS COLLATERAL AGENT
Reel/Frame 055194/0837 →
PATENT SECURITY AGREEMENT (UNITED STATES) Recorded Jun 23, 2020
From: NORSK TITANIUM AS
To: NTI HOLDING AS
Reel/Frame 053008/0564 →
INTELLECTUAL PROPERTY SECURITY AGREEMENT (UNITED STATES) Recorded Jun 23, 2020
From: NORSK TITANIUM AS
To: NTI HOLDING AS, AS COLLATERAL AGENT
Reel/Frame 053008/0932 →
SECURITY INTEREST Recorded May 19, 2020
From: NORSK TITANIUM AS
To: NTI HOLDING AS
Reel/Frame 052697/0362 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 31, 2016
From: HONEYWELL INTERNATIONAL INC.
To: NORSK TITANIUM AS
Reel/Frame 039605/0649 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 30, 2005
From: ADAMS, ROBBIE J.
To: HONEYWELL INTERNATIONAL, INC.
Reel/Frame 017327/0368 →