Method of drying a web
A method of drying a paper web is provided. The method utilizes a dryer, such as a through-dryer, having a first dryer section and a second dryer section. Within the first dryer section, a relatively wet paper web is dried at an elevated temperature, such as between about 400° F. to about 500° F. After being dried by the first dryer section, the web is relatively dry and is further dried by the second dryer section at a reduced temperature, such as between about 300° F. to about 400° F. A variety of control techniques can also be utilized to control the temperature of each dryer section.
1 - 33 . (canceled)
34 . A method for drying a wet web having a solids consistency of from about 20% to about 40%, the method comprising:
traversing the wet web through a first section of a through-air dryer, the first section being supplied with air heated to a temperature ranging from about 400° F. to about 500° C.; and
subsequently traversing the web through a second dryer section of the through-dryer, the second section being supplied with air heated to a temperature ranging from about 300° F. to about 400° C.
35 . The method of claim 34 , wherein the web is dried to a solids consistency of from about 45% to about 70% within the first section.
36 . The method of claim 34 , wherein the air supplied to the first section is heated to a temperature ranging from about 450° F. to about 500° F.
37 . The method of claim 34 , wherein the air supplied to the second section is heated to a temperature ranging from about 300° F. to about 350° F.
38 . The method of claim 34 , wherein the air is supplied to the first section at a relatively constant temperature.
39 . The method of claim 34 , wherein the air is supplied to the first section at a temperature that decreases as the web traverses therethrough.
40 . The method of claim 34 , wherein the air is supplied to the second section at a relatively constant temperature.
41 . The method of claim 34 , wherein the air is supplied to the second section at a temperature that increases as the web traverses therethrough.
42 . The method of claim 34 , wherein the web is a paper web comprising pulp fibers.
43 . The method of claim 34 , wherein the web is dried to a solids consistency of greater than about 90% within the second section.
44 . The method of claim 34 , wherein the web has a thermal degradation temperature, wherein the web is maintained below the thermal degradation temperature within the first section and the second section of the through-dryer.