Methods of rapidly simulating in-service warp distortion of a wood product and/or rapidly estimating shrinkage properties using electromagnetic energy

Assignee: Weyerhaeuser NR Company
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,584,652
App. No.
11/316,046
Granted
Sep 8, 2009
Kind
B2
Abstract

Methods are provided for rapidly simulating “in-service” warp distortion of a wood product. Methods are also provided for rapidly estimating shrinkage properties of a wood product by using electromagnetic energy to dry and redistribute absorbed water in the wood product.

Claims (23)

1. A method for rapid determination of a shrinkage rate coefficient for a wood product, the method comprising the steps of:

obtaining an initial moisture content “MC” and length “l” for the wood product;

generating an electromagnetic energy environment;

placing the wood product in the electromagnetic environment so that the wood product is subject to electromagnetic energy;

obtaining a change in length “Δl” and change in moisture content “ΔMC” for the wood product; and

obtaining a first longitudinal shrinkage rate coefficient LSRC 1 via the formula:

LSRC 1 =(Δ l/l )/Δ MC;

wherein the wood product is wrapped in a moisture barrier prior to being subjected to the electromagnetic energy.

2. The method of claim 1 wherein the electromagnetic energy is in the frequency range of 13.6 MHz (RF) to 2.45 GHz (microwave).

3. The method of claim 1 wherein the electromagnetic energy is in an RF range for inducing warp wherein the wood product is a full size lumber sample.

4. The method of claim 1 wherein the wood product is dried to a moisture content which is less than 20%.

5. A method for rapid determination of a shrinkage rate coefficient for a wood product, the method comprising the steps of:

obtaining an initial moisture content “MC” and length “l” for the wood product;

wrapping the wood product in a moisture barrier; thereafter

applying electromagnetic energy to the wood product; thereafter

obtaining a change in length “Δl” and change in moisture content “ΔMC” for the wood product; and

obtaining a first longitudinal shrinkage rate coefficient LSRC 1 via the formula: LSRC 1 =(Δl/l)/ΔMC.

6. A method for rapid determination of a shrinkage rate coefficient for a wood product, the method comprising the steps of:

obtaining an initial moisture content “MC i ” measurement and initial length “l i ” measurement for the wood product; thereafter

drying the wood product to a lower, subsequent moisture content “MC s ” by operating an electromagnetic energy source and directing the electromagnetic energy generated by the electromagnetic energy source at the wood product; thereafter obtaining a subsequent length “l s ” measurement and the subsequent moisture content “MC s ” for the wood product; and

obtaining a first longitudinal shrinkage rate coefficient LSRC 1 via the formula: LSRC 1 =(l i −l s /l i )/(MC i −MC s ).

7. The method of claim 6 wherein the wood product is wrapped in a moisture barrier prior to being subjected to the electromagnetic energy.

8. the method of claim 6 wherein the electromagnetic source as an RF dryer.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 21, 2009
From: WEYERHAEUSER COMPANY
To: WEYERHAEUSER NR COMPANY
Reel/Frame 022835/0233 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 19, 2006
From: FLOYD, STANLEY L.; HUANG, CHIH-LIN
To: WEYERHAEUSER COMPANY
Reel/Frame 017510/0124 →