IP Library Granted Patent US 7,455,739
Granted Patent B2
US 7,455,739 · App. 11/352,619 · Granted Nov 25, 2008

Shaped reinforcing member for medical device and method for making the same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,455,739
App. No.
11/352,619
Granted
Nov 25, 2008
Kind
B2
Abstract

Medical devices, medical device components, and methods of making the same. For example, one embodiment provides a method of shaping a reinforcing member through annealing. Another exemplary embodiment includes a method of making a medical device that includes such a shaped reinforcement member incorporated therein. Yet another exemplary embodiment provides a medical device including such a shaped reinforcing member therein.

Claims (30)

1. A method for manufacturing a medical device, the method comprising:

providing a reinforcing member consisting essentially of stainless steel, tungsten or combinations thereof;

applying a biasing force to the reinforcing member to bias the reinforcing member into a desired shape that includes a curve;

annealing the reinforcing member;

removing the biasing force, wherein the reinforcing member substantially maintains the desired shape when the biasing force is removed; and

disposing a tubular member on the reinforcing member, wherein the reinforcing member substantially maintains the desired shape when the tubular member is disposed on the reinforcing member such that the finished medical device maintains the desired shape.

2. The method according to claim 1 , wherein providing a reinforcing member includes providing a reinforcing braid.

3. The method according to claim 1 , wherein annealing the reinforcing member includes heating the reinforcing member at a temperature in the range of about 500° F. to about 1000° F.

4. The method according to claim 1 , wherein annealing the reinforcing member is performed over a time period in the range of about 0.25 to about 5 hours.

5. The method according to claim 1 , wherein annealing the reinforcing member includes removing internal strains in the reinforcing member caused by applying the biasing force to bias the reinforcing member into the desired shape.

6. The method according to claim 1 , wherein applying a biasing force to the reinforcing member to bias the reinforcing member into a desired shape that includes a curve includes loading the reinforcing member onto a mandrel.

7. The method according to claim 1 , wherein applying a biasing force to the reinforcing member to bias the reinforcing member into a desired shape that includes a curve includes loading the reinforcing member into a jig.

8. The method according to claim 1 , wherein the reinforcing member includes a proximal portion and a distal portion, and wherein the desired shape of the reinforcing member includes one or more curves formed in the distal portion.

9. The method according to claim 1 , further comprising disposing the reinforcing member about an inner tubular member.

10. A method for manufacturing a catheter, the method comprising:

providing a reinforcing member consisting essentially of stainless steel, tungsten or combinations thereof;

forming a curve in the reinforcing member;

annealing the reinforcing member;

disposing the annealed reinforcing member on a first tubular member; and

disposing a second tubular member on the annealed reinforcing member, wherein the curve formed in the annealed reinforcing member substantially maintains its shape when the second member is disposed on the annealed reinforcing member such that the finished catheter substantially maintains a desired shape.

11. The method according to claim 10 , wherein providing a reinforcing member includes providing a reinforcing braid.

12. The method according to claim 10 , wherein annealing the reinforcing member includes heating the reinforcing member at a temperature in the range of about 500° F. to about 1000° F.

13. The method according to claim 10 , wherein annealing the reinforcing member is performed over a time period in the range of about 0.25 to about 5 hours.

14. The method according to claim 10 , wherein annealing the reinforcing member includes removing internal strains in the reinforcing member caused by forming the curve in the reinforcing member.

15. A method for manufacturing a catheter, the method comprising:

providing a tubular reinforcing braid consisting essentially of stainless steel, tungsten or combinations thereof;

forming a curve in the tubular reinforcing braid;

annealing the tubular reinforcing braid;

disposing the annealed tubular reinforcing braid on a first tubular member; and

disposing a second tubular member on the annealed tubular reinforcing braid, wherein the curve formed in the annealed tubular reinforcing braid substantially maintains its shape when the second member is disposed on the annealed tubular reinforcing braid such that the finished catheter substantially maintains a desired shape.

Assignments (1)
CHANGE OF NAME Recorded Nov 6, 2006
From: SCIMED LIFE SYSTEMS, INC.
To: BOSTON SCIENTIFIC SCIMED, INC.