Processing asphaltene-containing tailings
View Patent ↗Embodiments of a method and a system for recovering energy, materials or both from asphaltene-containing tailings are disclosed. The asphaltene-containing tailings can be generated, for example, from a process for recovering hydrocarbons from oil sand. Embodiments of the method can include a flotation separation and a hydrophobic agglomeration separation. Flotation can be used to separate the asphaltene-containing tailings into an asphaltene-rich froth and an asphaltene-depleted aqueous phase. The asphaltene-rich froth, or an asphaltene-rich slurry formed from the asphaltene-rich froth, then can be separated into a heavy mineral concentrate and a light tailings. Hydrophobic agglomeration can be used to recover an asphaltene concentrate from the light tailings. Another flotation separation can be included to remove sulfur-containing minerals from the heavy mineral concentrate. Oxygen-containing minerals also can be recovered from the heavy mineral concentrate. Water removed by the various separation steps can be recycled and its heat energy recovered.
1. A method, comprising:
introducing gas into asphaltene-containing tailings such that asphaltenes in the asphaltene-containing tailings rise with bubbles of the gas to form an asphaltene-rich froth over an asphaltene-depleted aqueous phase comprising water and non-floatable minerals;
separating the asphaltene-rich froth, or an asphaltene-rich slurry formed from the asphaltene-rich froth, into a heavy mineral concentrate and a light tailings comprising water and asphaltenes;
dispersing a hydrophobic agglomeration agent within the light tailings to form droplets, wherein the droplets agglomerate with the asphaltenes to form asphaltene-containing particles; and
separating the asphaltene-containing particles from the light tailings as an asphaltene concentrate.
2. The method according to claim 1 , wherein the asphaltene-containing tailings comprise tailings from a process for recovering hydrocarbons from oil sand.
3. The method according to claim 1 , further comprising recovering heat energy from the asphaltene-depleted aqueous phase.
4. The method according to claim 1 , wherein separating the asphaltene-containing particles from the light tailings comprises separating the asphaltene-containing particles from the light tailings by gravity separation.
5. The method according to claim 1 , wherein separating the asphaltene-containing particles from the light tailings comprises separating the asphaltene-containing particles from the light tailings by filtration.
6. The method according to claim 1 , wherein the heavy mineral concentrate comprises titania, ilmenite, zirconia, or a combination thereof.
7. The method according to claim 1 , wherein the hydrophobic agglomeration agent comprises diesel, a fuel oil, a surfactant, or a combination or derivative thereof.
8. The method according to claim 1 , further comprising introducing a frother reagent comprising an aliphatic alcohol, a cyclic alcohol, a phenol, an alkoxy paraffin, a polyglycol, or a combination or derivative thereof, into the asphaltene-containing tailings before or while introducing gas into the asphaltene-containing tailings.
9. The method according to claim 1 , further comprising introducing a collector reagent comprising a fuel oil, sodium oleate, a fatty acid, a xanthate, an alkyl sulfuric salt, a dithiophosphate, an amine, or a combination or derivative thereof, into the asphaltene-containing tailings before or while introducing gas into the asphaltene-containing tailings.
10. The method according to claim 1 , further comprising introducing a dispersant reagent comprising a silicate, a phosphate, a citrate, a lignin sulfonate, or a combination or derivative thereof, into the asphaltene-rich froth or the asphaltene-rich slurry before or while separating the asphaltene-rich froth or the asphaltene-rich slurry into a heavy mineral concentrate and a light tailings.
11. The method according to claim 1 , further comprising introducing an oxidizing agent into the light tailings before or while dispersing the hydrophobic agglomeration agent.
12. The method according to claim 1 , further comprising introducing a causticizing agent into the light tailings before or while dispersing the hydrophobic agglomeration agent.
13. The method according to claim 1 , further comprising introducing an oxidizing agent and a causticizing agent or a mixture thereof into the light tailings before or while dispersing the hydrophobic agglomeration agent.
14. The method according to claim 1 , further comprising removing water from the asphaltene-rich froth or the asphaltene-rich slurry, and further comprising recovering heat energy from the water removed from the asphaltene-rich froth or the asphaltene-rich slurry.
15. The method according to claim 1 , further comprising separating coarse minerals from the asphaltene-containing tailings before introducing gas into the asphaltene-containing tailings.
16. The method according to claim 15 , wherein separating coarse minerals from the asphaltene-containing tailings comprises subjecting the asphaltene-containing tailings to a cyclone separation process, and the coarse minerals are removed with an underflow from the cyclone separation process.
17. The method according to claim 16 , wherein the cyclone separation process is a gas-sparged hydrocyclone separation process.
18. The method according to claim 1 , further comprising separating sulfur-containing minerals from the heavy mineral concentrate.
19. The method according to claim 18 , further comprising attritioning the heavy mineral concentrate before separating the sulfur-containing minerals from the heavy mineral concentrate.
20. The method according to claim 19 , wherein attritioning the heavy mineral concentrate comprises attritioning to clean the mineral surfaces.
21. The method according to claim 18 , wherein separating the sulfur-containing minerals from the heavy mineral concentrate comprises:
introducing gas into the heavy mineral concentrate such that the sulfur-containing minerals rise with bubbles of the gas to form a sulfur-rich froth over a sulfur-depleted aqueous phase comprising water and oxygen-containing minerals; and
recovering the oxygen-containing minerals from the sulfur-depleted aqueous phase.
22. The method according to claim 21 , further comprising recovering the sulfur-containing minerals from the sulfur-rich froth or a sulfur-rich slurry formed from the sulfur-rich froth.
23. The method according to claim 21 , wherein the oxygen-containing minerals comprise titania, ilmenite, zirconia, or a combination thereof.
24. The method according to claim 21 , further comprising introducing a frother reagent comprising an aliphatic alcohol, a cyclic alcohol, a phenol, an alkoxy paraffin, a polyglycol, or a combination or derivative thereof, into the heavy mineral concentrate before or while introducing gas into the heavy mineral concentrate.
25. The method according to claim 21 , further comprising introducing a collector reagent comprising a fuel oil, sodium oleate, a fatty acid, a xanthate, a alkyl sulfuric salt, a dithiophosphate, an amine, or a combination or derivative thereof, into the heavy mineral concentrate before or while introducing gas into the heavy mineral concentrate.
26. The method according to claim 1 , further separating a lignite concentrate from the asphaltene-rich froth or an asphaltene-rich slurry formed from the asphaltene-rich forth.
27. The method according to claim 26 , wherein separating the lignite concentrate comprises performing a screening process, a gravity separation process, a solvent extraction process or a combination thereof.
28. A method for recovering energy, materials or both from asphaltene-containing tailings, comprising:
introducing a hydrophobic agglomeration agent into tailings comprising water, asphaltenes and inorganic minerals;
dispersing the hydrophobic agglomeration agent to form droplets, wherein the droplets agglomerate with the asphaltenes to form asphaltene-containing particles; and
separating the asphaltene-containing particles from the tailings as an asphaltene concentrate.
29. The method according to claim 28 , wherein the asphaltene-containing tailings comprise tailings from a process for recovering hydrocarbons from oil sand.
30. The method according to claim 28 , wherein the hydrophobic agglomeration agent comprises diesel, a fuel oil, a surfactant, or a combination or derivative thereof.