IP Library Granted Patent US 7,575,773
Granted Patent B2
US 7,575,773 · App. 11/377,672 · Granted Aug 18, 2009

Optical compensatory sheet producing method and apparatus, thermal treating method and apparatus, and dust removing method and apparatus

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,575,773
App. No.
11/377,672
Granted
Aug 18, 2009
Kind
B2
Abstract

An optical compensatory sheet producing apparatus produces an optical compensatory sheet having a liquid crystal layer. In the apparatus, a rubbing unit is supplied with resin film having a first layer including resin, and subjects the first layer to a rubbing process, so as to form an orientation layer. A dust remover removes dust from the orientation layer by use of liquid such as perfluorocarbon, to which the orientation layer is insoluble. A liquid crystal layer coater is disposed downstream from the dust remover, for coating the orientation layer with coating liquid including liquid crystalline compound, so that the liquid crystal layer is formed.

Claims (6)

1. A thermal treating method for a dried coating layer, the coating layer formed by coating traveling web with coating liquid, comprising:

blowing said dried coating layer with hot air through an air blow opening; and sucking said hot air from said dried coating layer in a position upstream or downstream from said air blow opening according to a traveling direction of said web such that, while said hot air flows on said dried coating layer in the traveling director of said web, a flow speed of said hot air remaining equal to or lower than 1 m/sec with reference to a web width direction;

wherein said flow speed of said hot air in said web width direction is less than the flow speed of said hot air in said traveling direction of said web;

wherein said thermal treating is used in a process of forming a liquid crystal layer in a production of an optical compensatory sheet, and said coating contains a liquid crystalline compound.

2. The thermal treating method as defined in claim 1 , wherein a temperature of said hot air is in the range of 70° C. to 300° C.

3. The thermal treating method as defined in claim 1 , further comprising adjusting a moisture component included in said hot air.